Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00800 - 0.0120 cm/cm
0.00800 - 0.0120 in/in
ASTM D955
Niche Polymer PA66GM40BK Nylon 66, 40% Mineral Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00800 - 0.0120 cm/cm
0.00800 - 0.0120 in/in
ASTM D955
Niche Polymer PA66GM40N Nylon 66, 40% Mineral Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00800 - 0.0120 cm/cm
0.00800 - 0.0120 in/in
ASTM D955
Niche Polymer PPCT20BK Copolymer PP, 20% Talc Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00800 cm/cm
0.00800 in/in
ASTM D955
Niche Polymer PPHT40BK Homopolymer PP, 40% Talc Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.00800 - 0.0300 cm/cm
0.00800 - 0.0300 in/in
Average value: 0.0164 cm/cm Grade Count:29
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage 0.00800 - 0.0110 cm/cm

@Temperature 121 - 121 °C
0.00800 - 0.0110 in/in

@Temperature 250 - 250 °F
Average value: 0.00950 cm/cm Grade Count:1
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage 0.00800 - 0.0110 cm/cm

@Time 1800 - 1800 sec
0.00800 - 0.0110 in/in

@Time 0.500 - 0.500 hour
Average value: 0.00950 cm/cm Grade Count:1
Overview of materials for Polypropylene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage 0.00800 - 0.0250 cm/cm
0.00800 - 0.0250 in/in
Average value: 0.0131 cm/cm Grade Count:11
Overview of materials for Nylon 612, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.00800 - 0.0400 cm/cm
0.00800 - 0.0400 in/in
Average value: 0.0192 cm/cm Grade Count:26
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a..
Linear Mold Shrinkage 0.00800 - 0.0226 cm/cm
0.00800 - 0.0226 in/in
Average value: 0.0143 cm/cm Grade Count:26
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage 0.00800 - 0.0350 cm/cm
0.00800 - 0.0350 in/in
Average value: 0.0193 cm/cm Grade Count:33
Overview of materials for Acetal Copolymer, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage 0.00800 - 0.0160 cm/cm
0.00800 - 0.0160 in/in
Average value: 0.0109 cm/cm Grade Count:14
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..
Linear Mold Shrinkage 0.00800 - 0.0190 cm/cm
0.00800 - 0.0190 in/in
Average value: 0.0141 cm/cm Grade Count:35
Overview of materials for Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..