Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00100 - 0.00200 cm/cm
0.00100 - 0.00200 in/in
ASTM D955
Niche Polymer PPHT20BK Homopolymer PP, 20% Talc Fiber Filled
Information provided by Niche Polymer
Linear Mold Shrinkage 0.000500 - 0.00200 cm/cm
0.000500 - 0.00200 in/in
Average value: 0.00107 cm/cm Grade Count:4
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
Linear Mold Shrinkage 0.00100 - 0.00200 cm/cm
0.00100 - 0.00200 in/in
Average value: 0.00144 cm/cm Grade Count:6
Overview of materials for PPE/PPO + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPE/PPO + Carbon Fiber". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage 0.000500 - 0.00200 cm/cm
0.000500 - 0.00200 in/in
Average value: 0.00118 cm/cm Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 40% Glass Fiber Filled". Specific grades with glass content betwe..
Linear Mold Shrinkage 0.000500 - 0.00200 cm/cm
0.000500 - 0.00200 in/in
Average value: 0.00119 cm/cm Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Linear Mold Shrinkage 0.00100 - 0.00200 cm/cm
0.00100 - 0.00200 in/in
Average value: 0.00150 cm/cm Grade Count:3
Overview of materials for Polycarbonate, Carbon + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon + Glass Fiber Reinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.000 - 0.00200 cm/cm
0.000 - 0.00200 in/in
Average value: 0.000869 cm/cm Grade Count:12
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an..
Linear Mold Shrinkage 0.000100 - 0.00200 cm/cm
0.000100 - 0.00200 in/in
Average value: 0.000593 cm/cm Grade Count:15
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an..
Linear Mold Shrinkage 0.000 - 0.00200 cm/cm
0.000 - 0.00200 in/in
Average value: 0.000760 cm/cm Grade Count:5
Overview of materials for Phenolic, Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values ..
Linear Mold Shrinkage 0.000200 - 0.00200 cm/cm
0.000200 - 0.00200 in/in
Average value: 0.00110 cm/cm Grade Count:17
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Linear Mold Shrinkage 0.000500 - 0.00200 cm/cm
0.000500 - 0.00200 in/in
Average value: 0.000692 cm/cm Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Linear Mold Shrinkage 0.00200 - 0.00200 cm/cm

@Temperature 80.0 - 80.0 °C
0.00200 - 0.00200 in/in

@Temperature 176 - 176 °F
Average value: 0.00200 cm/cm Grade Count:6
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Linear Mold Shrinkage 0.000100 - 0.00200 cm/cm
0.000100 - 0.00200 in/in
Average value: 0.000875 cm/cm Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..
Linear Mold Shrinkage 0.00100 - 0.00200 cm/cm
0.00100 - 0.00200 in/in
Average value: 0.00175 cm/cm Grade Count:3
Overview of materials for Polyethylene Terephthalate (PET), 60% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 60% Glass Reinforced". Specific grades with glass content between 55% ..