Overview of materials for Nylon 12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Nylon 12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.820 - 11.0 g/cc
0.0296 - 0.397 lb/in³
Average value: 1.42 g/cc Grade Count:484
Filler Content 10.0 - 50.0 %
10.0 - 50.0 %
Average value: 28.5 % Grade Count:29
Apparent Bulk Density 0.215 - 0.425 g/cc
0.00777 - 0.0154 lb/in³
Average value: 0.361 g/cc Grade Count:8
Water Absorption 0.0500 - 3.50 %
0.0500 - 3.50 %
Average value: 1.00 % Grade Count:219
Moisture Absorption at Equilibrium 0.000 - 2.00 %
0.000 - 2.00 %
Average value: 0.590 % Grade Count:194
Water Absorption at Saturation 0.100 - 1.80 %
0.100 - 1.80 %
Average value: 1.31 % Grade Count:63
Additive Loading 2.00 - 30.0 %
2.00 - 30.0 %
Average value: 19.5 % Grade Count:8
Particle Size 4.00 - 100 µm
4.00 - 100 µm
Average value: 50.3 µm Grade Count:20
pH 4.00 - 6.00
4.00 - 6.00
Average value: 4.25 Grade Count:8
Specific Surface Area 1.00 - 9.00 m²/g
1.00 - 9.00 m²/g
Average value: 2.44 m²/g Grade Count:8
Viscosity Test 190 cm³/g
190 cm³/g
Average value: 190 cm³/g Grade Count:5
Thickness 140 - 660 microns
5.51 - 26.0 mil
Average value: 450 microns Grade Count:3
Linear Mold Shrinkage 0.000200 - 0.0200 cm/cm
0.000200 - 0.0200 in/in
Average value: 0.00679 cm/cm Grade Count:284
Linear Mold Shrinkage, Transverse 0.000500 - 0.0400 cm/cm
0.000500 - 0.0400 in/in
Average value: 0.00932 cm/cm Grade Count:180
Melt Flow 0.500 - 190 g/10 min
0.500 - 190 g/10 min
Average value: 26.5 g/10 min Grade Count:126
Mechanical Properties Metric English Comments
Hardness, Rockwell R 55.0 - 120
55.0 - 120
Average value: 104 Grade Count:36
Hardness, Shore D 40.0 - 88.0
40.0 - 88.0
Average value: 71.1 Grade Count:98
Ball Indentation Hardness 20.0 - 230 MPa
2900 - 33400 psi
Average value: 122 MPa Grade Count:59
Tensile Strength, Ultimate 17.0 - 827 MPa
2470 - 120000 psi
Average value: 79.8 MPa Grade Count:368
15.0 - 110 MPa

@Temperature 60.0 - 150 °C
2180 - 16000 psi

@Temperature 140 - 302 °F
Average value: 58.4 MPa Grade Count:4
Tensile Strength, Yield 9.50 - 170 MPa
1380 - 24600 psi
Average value: 45.8 MPa Grade Count:321
Elongation at Break 0.350 - 400 %
0.350 - 400 %
Average value: 53.7 % Grade Count:517
4.50 - 16.0 %

@Temperature 60.0 - 150 °C
4.50 - 16.0 %

@Temperature 140 - 302 °F
Average value: 8.68 % Grade Count:3
Elongation at Yield 1.50 - 45.0 %
1.50 - 45.0 %
Average value: 11.2 % Grade Count:205
>= 10.0 %

@Temperature 60.0 - 150 °C
>= 10.0 %

@Temperature 140 - 302 °F
Average value: 10.0 % Grade Count:1
Modulus of Elasticity 0.0800 - 64.1 GPa
11.6 - 9300 ksi
Average value: 5.35 GPa Grade Count:417
2.10 - 7.20 GPa

@Temperature 60.0 - 150 °C
305 - 1040 ksi

@Temperature 140 - 302 °F
Average value: 4.28 GPa Grade Count:3
Tenacity 0.297 - 0.545 N/tex
3.37 - 6.17 g/denier
Average value: 0.413 N/tex Grade Count:3
Flexural Yield Strength 5.45 - 607 MPa
790 - 88000 psi
Average value: 114 MPa Grade Count:182
Flexural Modulus 0.0100 - 51.7 GPa
1.45 - 7500 ksi
Average value: 5.34 GPa Grade Count:212
0.275 - 0.685 GPa

@Temperature 60.0 - 120 °C
39.9 - 99.4 ksi

@Temperature 140 - 248 °F
Average value: 0.450 GPa Grade Count:1
Compressive Yield Strength 38.0 - 110 MPa
5510 - 16000 psi
Average value: 71.0 MPa Grade Count:7
Izod Impact, Notched 0.160 - 100 J/cm
0.300 - 187 ft-lb/in
Average value: 2.23 J/cm Grade Count:170
0.210 - 1.10 J/cm

@Temperature -40.0 - -20.0 °C
0.393 - 2.06 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.410 J/cm Grade Count:5
Izod Impact, Unnotched 0.880 J/cm - NB
1.65 ft-lb/in - NB
Average value: 12.9 J/cm Grade Count:88
Izod Impact, Notched (ISO) 1.00 - 100000 kJ/m²
0.476 - 47600 ft-lb/in²
Average value: 13.2 kJ/m² Grade Count:40
Izod Impact, Unnotched (ISO) 8.00 kJ/m² - NB
3.81 ft-lb/in² - NB
Average value: 57.3 kJ/m² Grade Count:30
Charpy Impact Unnotched 0.500 J/cm² - NB
2.38 ft-lb/in² - NB
Average value: 6.83 J/cm² Grade Count:271
3.40 J/cm² - NB

@Temperature -40.0 - 30.0 °C
16.2 ft-lb/in² - NB

@Temperature -40.0 - 86.0 °F
Average value: 7.47 J/cm² Grade Count:193
Charpy Impact, Notched 0.100 J/cm² - NB
0.476 ft-lb/in² - NB
Average value: 1.96 J/cm² Grade Count:262
0.200 J/cm² - NB

@Temperature -40.0 - 30.0 °C
0.952 ft-lb/in² - NB

@Temperature -40.0 - 86.0 °F
Average value: 0.936 J/cm² Grade Count:226
Dart Drop, Total Energy 2.00 - 16.0 J
1.48 - 11.8 ft-lb
Average value: 9.54 J Grade Count:13
Falling Dart Impact 9.73 - 13.0 J
7.18 - 9.59 ft-lb
Average value: 11.2 J Grade Count:3
Coefficient of Friction 0.0200 - 0.670
0.0200 - 0.670
Average value: 0.301 Grade Count:17
Coefficient of Friction, Static 0.0800 - 0.520
0.0800 - 0.520
Average value: 0.285 Grade Count:10
Tensile Creep Modulus, 1 hour 310 - 1300 MPa
45000 - 189000 psi
Average value: 833 MPa Grade Count:8
Tensile Creep Modulus, 1000 hours 60.0 - 800 MPa
8700 - 116000 psi
Average value: 388 MPa Grade Count:12
Tear Strength Test 0.200 - 52.0
0.200 - 52.0
Average value: 19.1 Grade Count:3
K (wear) Factor 14.1 - 898 x 10-8 mm³/N-M
7.00 - 446 x 10-10 in³-min/ft-lb-hr
Average value: 131 x 10<sup>-8</sup> mm³/N-M Grade Count:8
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 1.00e+16 ohm-cm
1.00 - 1.00e+16 ohm-cm
Average value: 2.46e+14 ohm-cm Grade Count:270
Surface Resistance 1.00 - 5.20e+15 ohm
1.00 - 5.20e+15 ohm
Average value: 1.28e+14 ohm Grade Count:230
Insulation Resistance 10.0 - 1.00e+14 ohm
10.0 - 1.00e+14 ohm
Average value: 4.13e+12 ohm Grade Count:25
Static Decay 0.00200 - 2.00 sec
0.00200 - 2.00 sec
Average value: 1.50 sec Grade Count:4
Dielectric Constant 2.00 - 17.0
2.00 - 17.0
Average value: 4.90 Grade Count:82
Dielectric Strength 1.00 - 100 kV/mm
25.4 - 2540 kV/in
Average value: 33.0 kV/mm Grade Count:193
Dissipation Factor 0.000290 - 0.330
0.000290 - 0.330
Average value: 0.0665 Grade Count:82
Dielectric Loss Index 0.000200 - 0.0400
0.000200 - 0.0400
Average value: 0.0295 Grade Count:4
Comparative Tracking Index 60.0 - 600 V
60.0 - 600 V
Average value: 570 V Grade Count:171