Physical Properties Metric English Comments
Bulk Density 0.520 g/cc
0.0188 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons ECORAX® S 206 Carbon Black
Specialty black for tire treads and bodies that provide reduced rolling resistanceInformation provided by Orion Engineered Carbons.
Bulk Density 0.520 g/cc
0.0188 lb/in³
Pour Density; ASTM D 1513
Orion Engineered Carbons PUREX® LS 18 Carbon Black
Carbon black grade for manufactory of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons.
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D4894
3M Dyneon™ CC174-N PTFE, 15% Fiberglass/Moly Filled  (discontinued **)
Product Form: Gray, non-pelletized powder. Applications include bearings, rider rings, and packings.Data provided by Dyneon.
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D4745
3M Dyneon™ CC174/N Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of 15% fiberglass & 5% natural molybdenum disulfide blended with PTFE.Information provided by Dyneon, A 3M Company
Bulk Density 0.520 - 0.660 g/cc
0.0188 - 0.0238 lb/in³
ASTM D1895
LG Chemical LB110 PVC
General Description: LB110 is a homopolymer blending resin, which can be characterized with its fine particle size, medium molecular weight . It is used in plastically for viscosity , air released a..
Bulk Density 0.520 - 0.600 g/cc
0.0188 - 0.0217 lb/in³
ASTM D1895
LG Chemical LS080S PVC
General Description: LS080S, homopolymer made by suspension polymerization, can be applied to hard or semi-hard products.Main Applications: Hard sheets, films, fittings, injection molded products, b..
Bulk Density 0.520 - 0.600 g/cc
0.0188 - 0.0217 lb/in³
ASTM D1895
LG Chemical LS100E PVC
General Description: LS100E, homopolymer by mass polymerization, can be applied to various applications, such as semi rigid and rigid products.Main Applications: Pipe, profiles, sashCAS No: 9002-86-..
Bulk Density 0.520 g/cc
0.0188 lb/in³
DIN 53466
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound
TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP..
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Plenco 7500 Phenolic, Granular, Compression Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Plenco 7500 Phenolic, Granular, Injection Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Plenco 7500 Phenolic, Granular, Transfer Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
Bulk Density 0.520 g/cc
0.0188 lb/in³
Tap
TIMCAL TIMREX® GA95/75 Natural Graphite
TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-..
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Formosa Plastics Formolon® 676 PVC
Homopolymer General Purpose Grade Resin F676 is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered ..
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Plenco 7476 Phenolic, Granular, Transfer Molded
PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. ..
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Formosa Plastics Formolon® 622F PVC
Homopolymer Film Grade Resin F622F is a medium molecular weight PVC homopolymer suitable for both rigid extrusion applications and it is suitable for many flexible applications. This product has goo..
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Formosa Plastics Formolon® 676H PVC
Homopolymer General Purpose Grade Resin F676H is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered..
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Formosa Plastics Formolon® 685 PVC
Homopolymer General Purpose Grade Resin F685 is especially suited for processing from powder blends due to its ability to absorb plasticizers regardless of molecular weight. In addition, this produc..
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer
Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech..
Bulk Density 0.520 g/cc
0.0188 lb/in³
Asahi Glass Fluon® RB1020S 20% Glass Fiber, PTFE Filled Compound
Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc.
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Plenco 7697 Phenolic, Granular, Compression Molded
PLENCO 07697 is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for automotive pulleys. PLENCO 07697 is the same formulation as VALITE 697-A.Inform..