Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7500 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7500 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component file E40654. 07500 is available in black or red color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Water Absorption 0.49 %
0.49 %
ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 92
92
ASTM D785
Tensile Strength, Ultimate 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 0.76 %
0.76 %
ASTM D638
Tensile Modulus 9.10 GPa
1320 ksi
ASTM D638
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
Flexural Modulus 8.80 GPa
1280 ksi
ASTM D790
Compressive Strength 219 MPa
31800 psi
ASTM D695
Izod Impact, Notched 0.235 J/cm
0.440 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.233 J/cm²
1.11 ft-lb/in²
ASTM D256
Impact 172
172
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 61.0 µm/m-°C

@Temperature 40.0 - 130 °C
33.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.360 W/m-K

@Temperature 100 °C
2.50 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 196 °C
385 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 176 °C
349 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 25.3 %
25.3 %
ASTM D2863
Shrinkage 0.145 %
0.145 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.30e+12 ohm-cm
2.30e+12 ohm-cm
ASTM D247
Dielectric Constant 4.6
4.6
ASTM D150
Dielectric Strength 16.7 kV/mm
424 kV/in
Short Time; ASTM D149
Dissipation Factor 0.037
0.037
ASTM D150
Arc Resistance 88 sec
88 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638