Material Notes:
General Description: LB110 is a homopolymer blending resin, which can be characterized with its fine particle size, medium molecular weight . It is used in plastically for viscosity , air released and gloss control. The fine particle size makes it useful for producing thin applications.Main Applications: Plastically, Automotive underbody coater, Fabric coating, Flooring, Slush molding , DippingCAS No: 9002-86-2Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D790
Bulk Density 0.520 - 0.660 g/cc
0.0188 - 0.0238 lb/in³
ASTM D1895
Volatiles <= 0.40 %

@Temperature 110 °C,
Time 3600 sec
<= 0.40 %

@Temperature 230 °F,
Time 1.00 hour
ASTM D3030-90
Molecular Weight 60000 - 150000 g/mol
60000 - 150000 g/mol
Thermal Properties Metric English Comments
Melting Point 302 °C
576 °F
Descriptive Properties Value Comments
Autoignition Temperature 435°C
Degree of Polymerization 900-1000
30°C, JIS K 6720-2
K-Value 64
DIN53726 / ISO1628-2