Formosa Plastics Formolon® 676H PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded , PVC, Wire and Cable Grade
Manufacturer Formosa Plastics Corporation, USA
Trade Name Formolon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Formosa Plastics Formolon® 676H PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer General Purpose Grade Resin F676H is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered film, sheeting and blow molding.Applications: Calendering, Blown Flexible Films, Wire Insulation and Meat Wrap. ASTM Classification: GP4-15000, ASTM D1755Information provided by Formosa Plastics Corporation, USA
Physical Properties Metric English Comments
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Volatiles 0.20 %
0.20 %
ASTM D6980
Particle Mesh Size 40 Mesh
40 Mesh
99.9% thru; Malvern
200 Mesh
200 Mesh
4% thru; Malvern
Viscosity 0.95 cP
0.95 cP
Inherent; ASTM D5225
Relative Viscosity 2.27 cP
2.27 cP
Descriptive Properties Value Comments
Composition <1.0 ppm
Residual VCM, GC Head Space Method
10
Gel count, GP Gel Method
20
Contamination Count, OCS per 100g
K-Value 68
Fikentscher's Constant