Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 7500 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7500 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component file E40654. 07500 is available in black or red color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.36 %
0.36 %
ASTM D570
Linear Mold Shrinkage 0.0109 cm/cm
0.0109 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 87
87
ASTM D785
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 0.87 %
0.87 %
ASTM D638
Tensile Modulus 8.10 GPa
1170 ksi
ASTM D638
Flexural Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM D790
Compressive Strength 212 MPa
30700 psi
ASTM D695
Izod Impact, Notched 0.193 J/cm
0.362 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.186 J/cm²
0.885 ft-lb/in²
ASTM D256
Impact 115
115
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 43.0 µm/m-°C

@Temperature 40.0 - 130 °C
23.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 197 °C
387 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 151 °C
304 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Shrinkage 0.35 %
0.35 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+13 ohm-cm
5.00e+13 ohm-cm
ASTM D247
Dielectric Constant 4.3
4.3
ASTM D150
Dielectric Strength 11.3 kV/mm
287 kV/in
Short Time; ASTM D149
Dissipation Factor 0.044
0.044
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638