Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons ECORAX® S 206 Carbon Black Specialty black for tire treads and bodies that provide reduced rolling resistanceInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons PUREX® LS 18 Carbon Black Carbon black grade for manufactory of mechanical rubber goods such as extruded profiles and sealsInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D4894 |
3M Dyneon™ CC174-N PTFE, 15% Fiberglass/Moly Filled
(discontinued **) Product Form: Gray, non-pelletized powder. Applications include bearings, rider rings, and packings.Data provided by Dyneon. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D4745 |
3M Dyneon™ CC174/N Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 15% fiberglass & 5% natural molybdenum disulfide blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Bulk Density | 0.520 - 0.660 g/cc | 0.0188 - 0.0238 lb/in³ | ASTM D1895 |
LG Chemical LB110 PVC General Description: LB110 is a homopolymer blending resin, which can be characterized with its fine particle size, medium molecular weight . It is used in plastically for viscosity , air released a.. |
|||
Bulk Density | 0.520 - 0.600 g/cc | 0.0188 - 0.0217 lb/in³ | ASTM D1895 |
LG Chemical LS080S PVC General Description: LS080S, homopolymer made by suspension polymerization, can be applied to hard or semi-hard products.Main Applications: Hard sheets, films, fittings, injection molded products, b.. |
|||
Bulk Density | 0.520 - 0.600 g/cc | 0.0188 - 0.0217 lb/in³ | ASTM D1895 |
LG Chemical LS100E PVC General Description: LS100E, homopolymer by mass polymerization, can be applied to various applications, such as semi rigid and rigid products.Main Applications: Pipe, profiles, sashCAS No: 9002-86-.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | DIN 53466 |
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
Plenco 7500 Phenolic, Granular, Compression Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
Plenco 7500 Phenolic, Granular, Injection Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
Plenco 7500 Phenolic, Granular, Transfer Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | Tap |
TIMCAL TIMREX® GA95/75 Natural Graphite TIMREX Natural Flake Graphite is produced in a wide range of products distinguished by particle size distribution, chemistry and carbon content. Timcal mines the graphite from its own source in Lac-.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 676 PVC Homopolymer General Purpose Grade Resin F676 is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered .. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
Plenco 7476 Phenolic, Granular, Transfer Molded PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. .. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 622F PVC Homopolymer Film Grade Resin F622F is a medium molecular weight PVC homopolymer suitable for both rigid extrusion applications and it is suitable for many flexible applications. This product has goo.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 676H PVC Homopolymer General Purpose Grade Resin F676H is a medium molecular weight PVC homopolymer suitable for flexible applications and is exceptionally low in gels and finds wide acceptance in calendered.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
Formosa Plastics Formolon® 685 PVC Homopolymer General Purpose Grade Resin F685 is especially suited for processing from powder blends due to its ability to absorb plasticizers regardless of molecular weight. In addition, this produc.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech.. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | |
Asahi Glass Fluon® RB1020S 20% Glass Fiber, PTFE Filled Compound Fluon®PTFE FC has improved creep and wear resistance. A wide range of fillers such as glass fiber, graphite, bronze, carbon fiber are available. Information provided by Asahi Glass Company, Inc. |
|||
Bulk Density | 0.520 g/cc | 0.0188 lb/in³ | ASTM D1895 |
Plenco 7697 Phenolic, Granular, Compression Molded PLENCO 07697 is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for automotive pulleys. PLENCO 07697 is the same formulation as VALITE 697-A.Inform.. |