Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Glass Filled, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ CC174-N PTFE, 15% Fiberglass/Moly Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Form: Gray, non-pelletized powder. Applications include bearings, rider rings, and packings.Data provided by Dyneon.
Physical Properties Metric English Comments
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D4894
Density 2.27 g/cc
0.0820 lb/in³
ASTM D792
Particle Size 25 µm
25 µm
ASTM D4894
Deformation 3.0 %

@Pressure 15.00 MPa
3.0 %

@Pressure 2175 psi
ASTM D621
5.0 %

@Time 86400 sec,
Pressure 15.00 MPa
5.0 %

@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
value after 15 sec; ASTM D2240
67
67
initial value; ASTM D2240
Tensile Strength at Break 23.4 MPa
3390 psi
ASTM D4894
Elongation at Break 240 %
240 %
ASTM D4894
Tensile Modulus 0.152 GPa
22.0 ksi
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 101 µm/m-°C

@Temperature 30.0 - 100 °C
56.0 µin/in-°F

@Temperature 86.0 - 212 °F
ASTM E831
137 µm/m-°C

@Temperature 100 - 200 °C
76.0 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
171 µm/m-°C

@Temperature 200 - 300 °C
95.0 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity 0.270 W/m-K

@Temperature 250 °C
1.87 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
0.280 W/m-K

@Temperature 100 °C
1.94 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
Shrinkage 1.9 %
1.9 %
ASTM D4894