Material Notes:
PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. UL recognized under component file E40654. 07476 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.520 g/cc
0.0188 lb/in³
ASTM D1895
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.42 %
0.42 %
ASTM D570
Linear Mold Shrinkage 0.0058 cm/cm
0.0058 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 77
77
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Elongation at Break 1.0 %
1.0 %
ASTM D638
Tensile Modulus 6.90 GPa
1000 ksi
ASTM D638
Flexural Strength 81.0 MPa
11700 psi
ASTM D790
Flexural Modulus 7.00 GPa
1020 ksi
ASTM D790
Compressive Strength 189 MPa
27400 psi
ASTM D695
Poissons Ratio 0.35
0.35
ASTM D638
Shear Modulus 2.56 GPa
371 ksi
Calculated
Izod Impact, Notched 0.227 J/cm
0.425 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.264 J/cm²
1.26 ft-lb/in²
ASTM D256
Impact 169
169
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 44.0 µm/m-°C

@Temperature 40.0 - 130 °C
24.4 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 194 °C
381 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 196 °C
385 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Shrinkage 0.43 %
0.43 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.70e+11 ohm-cm
2.70e+11 ohm-cm
ASTM D247
Dielectric Constant 6.6
6.6
ASTM D150
Dielectric Strength 7.90 kV/mm
201 kV/in
Short Time; ASTM D149
Dissipation Factor 0.076
0.076
ASTM D150
Arc Resistance 159 sec
159 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638