Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Tedur® P 9529 PPS, ~55% Glass Fiber/Mineral (black only)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Manufacturer Albis Plastics
Trade Name Tedur®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® P 9529 PPS, ~55% Glass Fiber/Mineral (black only).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Compounded Regrind and/or Production Scrap, Excellent Cost-Performance Ratio. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Lamp Holders, Lamp SocketsProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
DIN 53 455
Modulus of Elasticity 17.0 GPa
2470 ksi
DIN 53 457
Flexural Yield Strength 135 MPa
19600 psi
DIN 53 452
Flexural Modulus 15.5 GPa
2250 ksi
DIN 53 457
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Albis North America Internal Test
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F