Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.00 - 2.10 g/cc | 0.0723 - 0.0759 lb/in³ | ASTM D792 |
Polikim EFALON® K-35 PTFE, 35% Carbon Filled K25 and K35 have less thermal expansion, higher wear resistance, less deformation under load properties compared to virgin Efalon® (PTFE). Applications: Bearings, piston rings, gaskets, seal rings... |
|||
Density | 0.000657 - 2.10 g/cc | 0.0000237 - 0.0759 lb/in³ | Average value: 1.16 g/cc Grade Count:154 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |
|||
Density | 1.64 - 2.10 g/cc | 0.0592 - 0.0759 lb/in³ | Average value: 1.85 g/cc Grade Count:35 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Density | 1.55 - 2.10 g/cc | 0.0560 - 0.0759 lb/in³ | Average value: 1.87 g/cc Grade Count:23 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
Density | 2.04 - 2.10 g/cc | 0.0737 - 0.0759 lb/in³ | extruded; ASTM D792 |
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high .. |
|||
Density | 2.04 - 2.10 g/cc | 0.0737 - 0.0759 lb/in³ | extruded; ASTM D792 |
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high .. |
|||
Density | 1.85 - 2.10 g/cc | 0.0668 - 0.0759 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATR 457© Phenolic Molding Glass fiber Filler, Compression Molded Characteristics:High shock resistant ( high impact strength ) High Mechanical StrengthHigh Dielectric StrengthHigh Electrical Insulation Color- pale brown Medium flow Applications:Electric motor en.. |
|||
Density | 1.90 - 2.10 g/cc | 0.0686 - 0.0759 lb/in³ | Molded |
Bulk Molding Compounds BMC T12-15526 General Purpose Molding Compound BMC T12-15526 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Density | 1.90 - 2.10 g/cc | 0.0686 - 0.0759 lb/in³ | ISO 1138 |
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat.. |