Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Albis Plastics Tedur® L V 9200-1 PPS, 60% Glass Fiber/Mineral  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Albis Plastics Tedur® L V 9200-1 PPS, 60% Glass Fiber/Mineral  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mineral-filled Grade with Improved Impact Strength, Low Mold Temp. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Shaft Seals, FlangesProcessing: Injection Molding (Melt Temperature: 610-645°F, Mold Temperature: 285°F)Tedur® is manufactured by Albis Plastics Corporation under license of the registered trademark owner (Bayer.) Data supplied by Albis Plastics Corporation.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
DIN 53 47
Mechanical Properties Metric English Comments
Tensile Strength at Break 180 MPa
26100 psi
DIN 53 455
Elongation at Break 1.7 %
1.7 %
DIN 53 455
Modulus of Elasticity 17.0 GPa
2470 ksi
DIN 53 457
Flexural Yield Strength 250 MPa
36300 psi
DIN 53 452
Flexural Modulus 17.0 GPa
2470 ksi
DIN 53 457
Compressive Yield Strength 172 MPa
24900 psi
ASTM D695
Izod Impact, Notched 2.99 J/cm
5.60 ft-lb/in
Approximation; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 V-0
V-0
Albis North America Internal Test
Processing Properties Metric English Comments
Melt Temperature 321 - 341 °C
610 - 646 °F
Injection
Mold Temperature 141 °C
286 °F