Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous filament strand from a pitch precursor.4000 filaments/strand, 97+% carbon assay, 11 µm filament diameter, 1.4 m/g yield, 0 tpm twist, 0.38 mm² fiber area in yarn cross section.Thornel® products were sold by Amoco and are now owned by Cytec.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
Specific Surface Area 0.70 m²/g
0.70 m²/g
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1400 MPa
203000 psi
Elongation at Break 0.90 %
0.90 %
Modulus of Elasticity 160 GPa
23200 ksi
In Tension
Thermal Properties Metric English Comments
Thermal Conductivity 22.0 W/m-K
153 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00130 ohm-cm
0.00130 ohm-cm
Users viewing this material also viewed the following: