BMC 0410 is a low profile BMC with zero shrinkage and low coefficient of thermal expansion. It is especially suited for precision mouldings in office and communication equipment. The combination of well-balanced mould ability with dimensional stability enables the design of complex shapes with highest dimension accuracy. To improve moulding we strongly recommend chrome-plated steel moulds and injector pins on male and female part.Information Provided by Menzolit
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
ISO 1183
Water Absorption <= 0.50 %
<= 0.50 %
ISO 62
Linear Mold Shrinkage -0.000500 cm/cm
-0.000500 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.0 MPa

@Temperature 22.0 °C
3920 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Tensile Strength, Yield 27.0 MPa

@Temperature 22.0 °C
3920 psi

@Temperature 71.6 °F
25mm flat samples, compression moulded; ISO 527-4
Elongation at Yield 0.00 %
0.00 %
tensile rupture strain; ISO 527-4
Modulus of Elasticity 14.0 GPa
2030 ksi
25mm flat samples, compression moulded; ISO 527-4
Flexural Strength 60.0 MPa

@Temperature 22.0 °C
8700 psi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 11.0 GPa

@Temperature 22.0 °C
1600 ksi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.30
0.30
Shear Modulus 5.40 GPa
783 ksi
in plane
Charpy Impact, Notched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 10.0 µm/m-°C
5.56 µin/in-°F
ISO 11359-2
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 150 °C
>= 302 °F
ISO 75-2
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 170 °C
338 °F
ISO 11357-2
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Oxygen Index 22 %
22 %
ISO 4589-2
Glow Wire Test 750 °C
1380 °F
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 30.0 kV/mm
762 kV/in
IEC 60243-1
Dissipation Factor 0.010
0.010
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 135 - 160 °C
275 - 320 °F
Injection moulding, matched metal die