IDI Composites W-102 Thermoset Polyester, Molding

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer IDI Composites
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IDI Composites W-102 Thermoset Polyester, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
Water Absorption 0.070 %
0.070 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.00050 - 0.0015 cm/cm
0.00050 - 0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 25 - 35
25 - 35
ASTM D2583
Tensile Strength, Ultimate 38.0 MPa
5510 psi
ASTM D638
Flexural Strength 97.0 MPa
14100 psi
ASTM D790
Compressive Strength 131 MPa
19000 psi
ASTM D695
Izod Impact, Notched 2.20 J/cm
4.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 12.6 kV/mm
320 kV/in
ASTM D149