Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycolac® INP449 ABS+SAN SABIC INP449 is a T-SAN (Teflon (PTFE)-Styrene-Ancrylonitrile) resin for use as an FR anti-drip agent |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Nilit FRIANYL B63 KV50 Nylon 6 for injection molding, 50% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | Dry As Molded |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, at 50% RH
(d AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal
(Unverified Data**) Delrin® FG400MTD BLA079 is a metal filled, medium viscosity acetal copolymer for injection molding. It is detected in metal detectors. It has been developed for consideration into applications such.. |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds RH 225 Rigid PVC, Antishock Extrusion Antishock pipes and profiles |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI LNP* LUBRICOMP* EX06405 is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible, Easy Molding. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP EX06405 PEI (Asia Pacific) LNP* Lubricomp* EX06405 is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched LNP* LUBRICOMP* OCP36A is a compound based on PPS - Branched resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific) LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Valox® 420 PBT 30% GR, excellent strength, stiffness and dimensional stability. High heat resistance. Appliance handles, spotlights, electric motors, connectors. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Techmer ES HiFill® PBT GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: Natural ColorTPCI# 8649111Information provided by TP Composites, Inc. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF009S PA 66 LNP* THERMOCOMP* RF009S is a compound based on Nylon 66 resin containing 45% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM CO GF20 UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 20% Filler by WeightAdditive: UV StabilizerFeatures: Copolymer and Chemically CoupledAppearance: BlackInformati.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp LFZ42XXC PEEK LNP THERMOCOMP* LFZ42XXC is a compound based on Polyetheretherketone resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage.This data was supplied by SABIC.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Plenco 7507 Phenolic, Granular, Transfer Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | DIN 53479 |
Polyram RamSter PE300J6 PET, 30% Glass Fiber and Glass Bead Reinforced 30% Glass-fiber and glass beads reinforced, high stiffness PET for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 2754 Two-Component Epoxy Flexible Low-Stress Encapsulant Emerson & Cuming 2754 Stycast® Two-Component Epoxy Flexible Low-Stress EncapsulantDescriptionElectronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive compo.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | dry; ISO 1183 |
DSM Stanyl® SC50 PA46-GF30 FR 30% Glass Reinforced, Flame Retardant, Halogen free and free of red phosphorous |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NB40 GR15 NL XA70 PA6, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1183 |
Fainplast Compounds CKL 86 Flexible PVC, Sheathing Lead Free General purposes |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® P123WO PBT Polyester, 15% Glass Reinforced PBT polyester with 15% glass reinforcement, flame retardant.Data provided by the manufacturer |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Azoty Tarnow™ TARNOFORM 300 GB4 POM 20% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | |
A. Schulman ComAlloy Lubrilon® 620 Nylon 6/6, Glass Fiber/Molybdenum Disulfide Filled, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Techmer ES Statiblend® PPS GF23 IM BK 23% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 23% Filler by WeightAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided.. |