Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792, ISO 1183
Nilit Nilitop BT G4 FR C3 is a 20% Glass Fiber Reinforced, Flame Retardant PBT
Description: Nilitop BT G4 FR C3 is a 20% glass fiber reinforced, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive. It..
Density 1.52 g/cc

@Temperature 23.0 °C
0.0549 lb/in³

@Temperature 73.4 °F
ISO 1183
PolyOne Bergamid™ B70 G45 BK Polyamide 6 (Nylon 6)
Information provided by PolyOne
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP CZL36 PS
LNP LUBRICOMP* CZL36 is a compound based on Polystyrene resin containing 30% Milled Glass and 15% PTFE. Added features of this material include: Internally Lubricated.
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Plenco 7300 Phenolic, Nodular, Injection Molded  (discontinued **)
Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file..
Density 1.52 g/cc
0.0549 lb/in³
DIN 53479; ASTM D792
Kolon SPESIN® KP213G30 Flame Retardant PBT Resin
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High..
Density 1.52 g/cc
0.0549 lb/in³
DIN 53479; ASTM D792
Kolon SPESIN® KP513G30WBL Multi Reinforced PBT Resin
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High..
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Density 1.52 g/cc
0.0549 lb/in³
Momentive Performance Materials Ultraglaze® 4000 Construction Sealant
High strength, one-part structural glazing/weathersealing system. Cure Method: Alkoxy (Neutral). Tack-free time 2 to 5 hr. Sag/slump 0.1 in.Data provided by the manufacturer, GE Silicones.GE Sili..
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP RFL36L PA 66 (Asia Pacific)
LNP* Lubricomp* RFL36L is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Techmer ES Electrablend® PCA 06006 BK Nickel-Coated Carbon Fiber/Stainless Steel Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Nickel-Coated Carbon Fiber and Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI)Appearance: BlackTPCI# 9691124Information ..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics ULTEM SF2350 PEI Blend
High flow Ultem blends for thin wall application
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP D451 PC (Asia Pacific)
LNP* Thermocomp* D451 (or EXTC8141) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good duc..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp KF003 Acetal Copoly
LNP* Thermocomp* KF003 is a compound based on Acetal Copolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
SABIC Innovative Plastics LNP Thermocomp PFB139E PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PFB139E is a compound based on PA 6 resin containing Glass Fiber, Glass Bead, Flame Retardant. Added features include; Flame Retardant, Easy Molding.This data was supplied by SABIC-..
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI
LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features include: Healthcare.
Density 1.52 g/cc
0.0549 lb/in³
Cosmic Plastics ID-40 Orlon Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Density 1.52 - 1.55 g/cc
0.0549 - 0.0560 lb/in³
Chengdu Polyster RPM650 Flame Retardant Masterbatch
RPM650 is a red phosphorus based additive flame retardant designed foruse in polyethylene resins. It is halogen free and has good flame retardant performance. Red pellet form. Wire insulation, elect..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
DSM Arnite® TV8 260 PBT-30% Glass Reinforced (European Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® SK605 BK851 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 BK851 is a 30% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Ensinger Tecapeek® XP-90 Compression Molded PEEK Compound, 25% Fiberglass
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Density 1.52 - 1.56 g/cc
0.0549 - 0.0564 lb/in³
ISO R 1183
Fainplast Compounds GA 80 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Eurotec® Tecomid® NA40 KC50 BK111 PA6.6, 50% glass/carbon fiber reinforced, black
Information provided by Eurotec®
Density 1.52 - 1.56 g/cc
0.0549 - 0.0564 lb/in³
ISO R 1183
Fainplast Compounds AP 95/1 Flexible PVC, Flame Retardant Insulation
General purposes
Density 1.52 g/cc
0.0549 lb/in³
cured 14 days @ 50% RH
3M AC-730 Class B-2 Aerospace Sealant
3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca..
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Celanese CELANEX 1462Z PBT, 30% Glass Reinforced
Celanex 1462Z is a general purpose, 30% glass reinforced polybutylene terephthalate with a good balance of mechanical properties and processability.Information provided by Celanese
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Celanese Celstran® PP-GF45M15-04CN15/10 PP, 60% Mineral / Glass Reinforced
Material code according to ISO 1043-1: PPInformation provided by Celanese
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183
Celanese Celstran® TPU-GF40-01-US TPU, 40% Glass Reinforced
40% long strand glass fiber reinforced thermoplastic polyurethaneInformation provided by Celanese
Density 1.52 g/cc
0.0549 lb/in³
ISO 1183