Material Notes:
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 1.44 - 1.56 g/cc
0.0520 - 0.0564 lb/in³
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 6.50 - 9.50 MPa
943 - 1380 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.860 - 1.06 W/m-K

@Temperature 600 °C
5.97 - 7.36 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.890 - 1.09 W/m-K

@Temperature 1000 °C
6.18 - 7.56 BTU-in/hr-ft²-°F

@Temperature 1830 °F
0.900 - 1.10 W/m-K

@Temperature 200 °C
6.25 - 7.63 BTU-in/hr-ft²-°F

@Temperature 392 °F
Maximum Service Temperature, Air 1800 °C
3270 °F
Shrinkage 0.200 - 0.400 %

@Temperature 1650 °C,
Time 86400 sec
0.200 - 0.400 %

@Temperature 3000 °F,
Time 24.0 hour
Component Elements Properties Metric English Comments
Al2O3 99 %
99 %
Fe2O3 0.10 %
0.10 %
SiO2 0.20 %
0.20 %
Descriptive Properties Value Comments
Segercone 42