Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.53 g/cc | 0.0553 lb/in³ | STN 64 0111 |
Plastcom SLOVAMID 66 W 40 Polyamide 66, 40% Mineral Filled FeaturesPA 66 with the content of 40% chemically modified mineral filler. Used for grips of electric hand tools, hobby tools, gear wheels, covers of electric tools, flat products, automobile wheel .. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | molded; ISO 1183 |
SABIC Innovative Plastics Cycolac® INP449 SAN SABIC INP449 is a T-SAN (Teflon (PTFE)-Styrene-Ancrylonitrile) resin for use as an FR anti-drip agentThis data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Polykemi AB POLYshine PBT D223 Q30 FR PBT, Mineral Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds RH 225 Rigid PVC, Antishock Extrusion Antishock pipes and profiles |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific) LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp RL0049 PA 66 LNP* Lubricomp* RL0049 is a compound based on Nylon 66 resin containing PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant.This data was supplied.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS (Asia Pacific) LNP* Stat-kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Techmer ES HiFill® PBT GF30 BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAppearance: BlackTPCI# 9864111Information provided by TP Composites, Inc. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific) LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF00469S PA 66 (Asia Pacific) LNP* Thermocomp* RF00469S is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF009H PA 66 (Asia Pacific) LNP* Thermocomp* RF009H is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ASTM D792 |
Techmer ES HiFill® POM CO GF20 UV BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 20% Filler by WeightAdditive: UV StabilizerFeatures: Copolymer and Chemically CoupledAppearance: BlackInformati.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Polyplastics Duranex® 303RA Polybutylene Terephthalate (PBT), Resin adhesion improved for multiple injection molding, 30% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | Relative Density; ISO 1183 |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | DIN 53479 |
Polyram RamSter PF320G3 PBT, 15% Glass Fiber, Flame Retardant 15% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol.. |
|||
Density | 1.53 - 2.03 g/cc | 0.0553 - 0.0733 lb/in³ | |
Trelleborg Offshore Vikotherm™ 73780 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 78 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR15 BK002 XA21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.53 - 1.57 g/cc | 0.0553 - 0.0567 lb/in³ | ISO R 1184 |
Fainplast Compounds R 220/R Rigid PVC, Extrusion Shiny rolling shutters |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® FG400MTD BLA079 Acetal (POM)
(Unverified Data**) Metal Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400MTD BLA079 is a metal filled medium viscosity acetal copolymer for injection molding. It is det.. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | |
Arkema Group Nakan® RPS 400 M PVC, Rigid Extrusion Grade NAKAN RPS 400 M is a rigid polyvinyl chloride compound developed for extrusion of cables ducts.ISO data provided by the manufacturer, Arkema. |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
BASF Ultradur B 4300 G6 BKQ16 15007 PBT |
|||
Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® HT1V-4 HY black 9205 PA6T/6I-GF40 Product description: Grivory HT1V-4 HY black 9205 is a 40% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-4 HY bl.. |