Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Alathon® L5332CP High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer LyondellBasell (former Equistar)
Trade Name Alathon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Alathon® L5332CP High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsALATHON L 5332CP, formerly known as LYHD 048, is designed to meet the requirements of AAHTO M294 stress crack resistance. It exhibits excellent processing stability and high crush resistance. Typical applications include corrugated pipe, conduit and profile extruded applications. L 5332CP conforms to ASTM D 3350 cell classification. NCTL > 24 hrs per AASHTO M294.Regulatory StatusL 5332CP meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "…articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.ProcessingSpecific recommendations for processing L 5332CP can only be made when the processing conditions, equipment and end use are known.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 0.32 g/10 min
0.32 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength at Break 36.5 MPa
5300 psi
ASTM D638
Tensile Strength, Yield 22.4 MPa
3250 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
1% Secant Modulus 1230 MPa
179000 psi
ASTM D790
Tensile Impact 152 J/cm
285 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C
144 °F
ASTM D648
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Users viewing this material also viewed the following: