ExxonMobil Escorene® AD2528 Adhesive Application Resin

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Exxon Chemical
Trade Name Escorene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene® AD2528 Adhesive Application Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Escorene Ultra AD 2528 is a very high flow rate, 27.6% Vinyl Acetate, copolymer, which is useful in formulating hot melt adhesives.Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsViscosity ModifierHot Melt AdhesivesWax BlendsPackaging AdhesivesInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ExxonMobil Method
Viscosity 2800 cP

@Temperature 190 °C
2800 cP

@Temperature 374 °F
ASTM D3236
Vinyl Acetate Content 27.6 %
27.6 %
ExxonMobil Method
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
15s; ASTM D2240
Hardness, Shore D 15
15
15s; ASTM D2240
Tensile Strength at Break 2.00 MPa
290 psi
ASTM D638
Elongation at Break 240 %
240 %
ASTM D638
Flexural Modulus 0.0276 GPa
4.00 ksi
1% secant; ASTM D790
Thermal Properties Metric English Comments
Melting Point 73.9 °C
165 °F
Peak Melting Temperature; ExxonMobil Method