Material Notes:
Product Description: AA53-003 is a pipe extrusion grade high density polyethylene copolymer offering an excellent combination of stiffness and stress crack resistance. This material meets or exceeds the AASHTO M294 requirement.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: No Applications: Drainage PipesFood packagingHigh Drainage PipeInformation provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ASTM D4883
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
High Load Melt Index 26 g/10 min

@Load 21.6 kg,
Temperature 190 °C
26 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
ASTM D638
2% Secant Modulus 1.24 GPa
180 ksi
Flexural; ASTM D790
Processing Properties Metric English Comments
Melt Temperature 177 °C
350 °F
Descriptive Properties Value Comments
Notched Constant Ligament Stress >24 hrs
ASTM F2136