Borealis BorSafe™ HE3495-LS HDPE Compound

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Borealis
Trade Name BorSafe™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BorSafe™ HE3495-LS HDPE Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BorSafe™ HE3495-LS is a bimodal polyethylene compound produced by the advanced Borstar® technology. It's fully stabilized against thermal degradation and the die build-up during extrusion is minimized. Furthermore, it has a highly covered pigment that gives a bright colored stripe even when extruded as a thin layer on a black pipe. It also contains UV-stabilizer. Applications: BorSafe™ HE3495-LS recommended for the production of identifying stripes of black pipes produced from BorSafe™ HE3490-LSInformation provided by Borealis AG
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ISO 1183
Melt Flow 0.30 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133