Physical Properties Metric English Comments
Density 0.926 - 0.960 g/cc
0.0335 - 0.0347 lb/in³
Average value: 0.942 g/cc Grade Count:51
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported..
Density 0.880 - 0.960 g/cc
0.0318 - 0.0347 lb/in³
Average value: 0.924 g/cc Grade Count:71
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Density 0.947 - 0.960 g/cc
0.0342 - 0.0347 lb/in³
ASTM D792
Forever Plast Namtene® Recycled Standard HDPE
Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications.
Density 0.953 - 0.961 g/cc
0.0344 - 0.0347 lb/in³
ASTM D792-98
Ipiranga Petrochem GM 5240 PR HDPE
IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce ..
Density 0.900 - 0.960 g/cc
0.0325 - 0.0347 lb/in³
ASTM D 792
Karina 6122/23-RTR Kariprene Crepe
Thermoplastic rubber compound recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Density 0.900 - 0.960 g/cc
0.0325 - 0.0347 lb/in³
ASTM D 792
Karina 6125/1-RTR Kariprene Natural
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Density 0.900 - 0.960 g/cc
0.0325 - 0.0347 lb/in³
ASTM D 792
Karina 6148/1-RTR Kariprene Black
Thermoplastic rubber compound, recommended for injection of footwear soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Density 0.940 - 0.960 g/cc
0.0340 - 0.0347 lb/in³
RPC-11002
Solvay DURAPHOS® 178 Surfactant
Identification: ALKYL AMINE NEUTRALIZED ORGANIC PHOSPHATECAS: 68187-67-7Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: DURAPHOS© 178 is a concentrated amine neut..
Density 0.801 - 0.961 g/cc
0.0289 - 0.0347 lb/in³
Dry
Unifrax Fiberfrax® Vari-Form™ B Casting Mix
Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu..
Density 0.801 - 0.961 g/cc
0.0289 - 0.0347 lb/in³
CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated
HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntact..
Density 0.960 - 0.960 g/cc

@Temperature 290 - 290 °C
0.0347 - 0.0347 lb/in³

@Temperature 554 - 554 °F
Average value: 0.960 g/cc Grade Count:1
Overview of materials for Nylon 6, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri..