Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SIDPEC EGYPTENE® HD 5301 EA HDPE Blow Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer SIDPEC (Sidi Kerir Petrochemicals Co.)
Trade Name EGYPTENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SIDPEC EGYPTENE® HD 5301 EA HDPE Blow Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:High performance blow molded containers typically of to 60 liters capacity for packaging aggressive productsRobust industrial and technical moldingsInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products
Physical Properties Metric English Comments
Density 0.953 g/cc
0.0344 lb/in³
ISO 1872/1
ESCR, Bottle 75 hour

@Temperature 50.0 °C
75 hour

@Temperature 122 °F
BP 13C/25
High Load Melt Index 11 g/10 min

@Load 21.6 kg
11 g/10 min

@Load 47.6 lb
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
BP 13B/1
Elongation at Break 1000 %
1000 %
BP 13B/1
Flexural Modulus 0.900 GPa
131 ksi
ISO 178-1975
Impact 4.4
4.4
M, F50; BP 13B/11