Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D792 |
Polimeros Mexicanos Rotolene® Black Plus Polyethylene Polyethylene compound specially formulated for rotational molding applications requiring good mechanical properties and good mold release properties. Rotational molded parts have smooth surface and .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | Exxon Method |
ExxonMobil Escorene® MV-02528 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 27.5% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HL3721 Sheet and Thermoforming HDPE
(discontinued **) Medium Density Hexene CopolymerApplications: Geomembranes, gas and chemical tank containment liners, landfill liners.Formolene HL3721 is tailored for extrusion applications requiring good processabi.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HL3712 Sheet and Thermoforming HDPE
(discontinued **) Medium Density Hexene CopolymerApplications: Gas and chemical tank containment liners, pond liners, landfill liners, tunnel liners.Formolene HL3712 has good processability, excellent melt strength, .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM TR-400G Medium density hexene copolymer
(discontinued **) Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: pond liners, gas and chemical tank containment liners, landfill liner.. |
|||
Density | 0.937 - 1.06 g/cc | 0.0339 - 0.0383 lb/in³ | Average value: 0.957 g/cc Grade Count:19 |
Overview of materials for High Density Polyethylene (HDPE), Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Sheet/Thermoforming Grade". Each property range of values reported is .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Braskem LH 437 LMDPE Cast Film Extrusion Polyethylene
(discontinued **) Applications: Diapers (back sheet); Absorbent pads (back sheet). Information provided by Braskem |
|||
Density | 0.937 - 0.945 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez 298-285 High Density Polyethylene Composite Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-.. |
|||
Density | 0.937 - 0.943 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez PE80B-285 High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.937 - 0.943 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez PE80B-285D High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.937 - 0.943 g/cc | 0.0339 - 0.0341 lb/in³ | |
Kazanorgsintez PE80B-285SL High Density Polyethylene Composite, Film Grade Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D4883 |
Ineos G36-24-150 HDPE Ineos G36-24-150 is a medium density polyethylene resin designed for geomembrane sheet extrusion. The resin has excellent environmental stress crack resistance (ESCR).Natural resin; some physical p.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | compound; ISO 1872-2/ISO 1183 |
Borealis Borcell™ ME1244 Medium Density Polyethylene Borcell™ ME1244 is a fully formulated compound for chemical foamed telesingles. ME1244 is a medium-density polyethylene compound containing chemical blowing agent. Applications Borcell™ ME1244 i.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D792-ISO 1183 |
DuPont Elvax® 420 Ethylene Vinyl Acetate DuPont™ Elvax® 420 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 420 resins can be used for the following applications: adhesives, sealants.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® HF3728 Film (Hexene) HDPE High Density Polyethylene Medium Molecular weight Film Resin Formolene® HF3728 is a medium density resin that provides an excellent overall balance of tensile, impact, and tear properties in thin f.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: geomembrane, gas and chemical containment liners, landfill linersInfor.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® K306 Fully Formulated Medium Density Hexene Copolymer Fully Formulated Medium Density Hexene CopolymerCustomer Benefits: This extrusion grade hexene copolymer has good processability, excellent melt strength, broad fusion range, outstanding ESCR, meets.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® K307 MDPE Hexene Copolymer Extrusion grade hexene copolymerCharacteristics: good processability, excellent melt strength, broad fusion range, outstanding stress crack resistance, meets the requirements of GRI-GM13. Meets A.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ FL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00014 is a copolymer of ethylene and vinyl acetate. For film requiring very high toughness, low creep, excellent optical properties and low gel.Availability: Africa & Middle .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00014 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil Escorene™ UL 53019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 53019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® E589 Polymer Modifier DuPont™ Fusabond® E589 is an anhydride modified polyethylene. Uses: Adhesives Pipe Coating Tie-Layer Features premium adhesive for Pipe Coating tie-layer at high surface temperatures. ( 90°C) |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 8450.31 Linear Low Density Polyethylene Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM-D792 |
Braskem LH537 LLDPE Cast Film Extrusion Polyethylene LH537 is a LLDPE Hexene produced by Braskem. It offers an excellent processability, stiffness, and soft touch for flat die films. It has very low gel contents. It contains slip absent and antiblock .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ASTM D 792 |
Total Finathene® HL 328 HDPE resin
(discontinued **) Applications: Specialty merchandise bags, millinery/notion bags, mailing envelopes, heavy-duty shipping sacks, shrink films, fresh cut produce packaging, coextrusionInformation provided provided by .. |
|||
Density | 0.937 g/cc | 0.0339 lb/in³ | ISO 1183 |
Borealis Borstar® FB4370 Medium Density Polyethylene Borstar® FB4370 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Applications: Borstar® FB4370 has been developed especially for ap.. |