ExxonMobil Escorene™ FL 00014 Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ FL 00014 Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: FL 00014 is a copolymer of ethylene and vinyl acetate. For film requiring very high toughness, low creep, excellent optical properties and low gel.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Bag in BoxBatch Inclusion BagsBlown FilmFood packagingProtective FilmInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ExxonMobil method
Vinyl Acetate Content 14 %
14 %
ExxonMobil method
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 600 %
600 %
ASTM D882
Film Elongation at Break, TD 650 %
650 %
ASTM D882
Film Tensile Strength at Break, MD 33.8 MPa
4900 psi
ASTM D882
Film Tensile Strength at Break, TD 35.9 MPa
5200 psi
ASTM D882
1% Secant Modulus, MD 82.7 MPa
12000 psi
ASTM D882
1% Secant Modulus, TD 89.6 MPa
13000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 193 °C
<= 379 °F
Peak Melting Point; ExxonMobil method
Vicat Softening Point 76.1 °C
169 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 4.5 %
4.5 %
ASTM D1003
Gloss 72 %
72 %
45°; ASTM D2457