Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® K307 MDPE Hexene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® K307 MDPE Hexene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion grade hexene copolymerCharacteristics: good processability, excellent melt strength, broad fusion range, outstanding stress crack resistance, meets the requirements of GRI-GM13. Meets ASTM D4976-89 - PE 235. ASTM D1248 - Type II, Class A, Category 5. Applications: pond liners, gas and chemical tank containment liners, landfill linersData provided by Chevron Phillips Chemical Company, LP.
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ASTM D1505
ESCR 100% Igepal® >= 1500 hour
>= 1500 hour
Cond. C; 100% Igepal®; F<sub>50</sub>; ASTM D1693
>= 1500 hour
>= 1500 hour
Cond. B; 10% Igepal®; F<sub>50</sub>; ASTM D1693
High Load Melt Index 21 g/10 min

@Load 21.6 kg,
Temperature 190 °C
21 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
Type IV; 50 mm per min crosshead speed; ASTM D638
Elongation at Break >= 700 %
>= 700 %
Type IV; 50 mm per min crosshead speed; ASTM D638
Flexural Modulus 0.834 GPa
121 ksi
ASTM D790
Processing Properties Metric English Comments
Processing Temperature 193 - 232 °C
379 - 450 °F
Extrusion Stock