Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® K306 Fully Formulated Medium Density Hexene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Extruded
Manufacturer Chevron Phillips Chemical Company LP
Trade Name Marlex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® K306 Fully Formulated Medium Density Hexene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fully Formulated Medium Density Hexene CopolymerCustomer Benefits: This extrusion grade hexene copolymer has good processability, excellent melt strength, broad fusion range, outstanding ESCR, meets the requirements of GRI-GM12Applications: Recommended rein for pond liners, gas and chemical tank containment liners, landfill liners.Processing Recommendations:Extrusion Melt Temperature: Upper Limit: 232°C, Lower Limit: 193°CSpecification Data: ASTM D1248 - Type III, Class A, Category 5. ASTM D4976-89 PE 225Data provided by Chevron Phillips Chemical Company, LP.
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 1500 hour
1500 hour
Condition C (100% Igepal), F<sub>50</sub>, ASTM D1693; Condition B (10% Igepal), F<sub>50</sub>: 1500, ASTM D1693
Melt Flow 12 g/10 min
12 g/10 min
Condition 190/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 19.0 MPa
2760 psi
2 in per min; ASTM D638 Type IV
Elongation at Break >= 700 %
>= 700 %
2 in per min; ASTM D638 Type IV
Flexural Modulus 0.800 GPa
116 ksi
ASTM D790
Processing Properties Metric English Comments
Processing Temperature 193 - 232 °C
379 - 450 °F
Extrusion