Physical Properties Metric English Comments
Density 0.940 - 0.944 g/cc
0.0340 - 0.0341 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4142L (424F5) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.940 - 0.944 g/cc
0.0340 - 0.0341 lb/in³
Base Resin; ASTM D1505
NIZHNEKAMSKNEFTEKHIM PE 4143L (424F5) High Density Polyethylene
Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer
Density 0.937 - 0.945 g/cc
0.0339 - 0.0341 lb/in³
Kazanorgsintez 298-285 High Density Polyethylene Composite
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-..
Density 0.937 - 0.945 g/cc
0.0339 - 0.0341 lb/in³
Kazanorgsintez 298-285D High Density Polyethylene Composite
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions 296-..
Density 0.937 - 0.943 g/cc
0.0339 - 0.0341 lb/in³
Kazanorgsintez PE80B-285 High Density Polyethylene Composite, Film Grade
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are ..
Density 0.937 - 0.943 g/cc
0.0339 - 0.0341 lb/in³
Kazanorgsintez PE80B-285D High Density Polyethylene Composite, Film Grade
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are ..
Density 0.937 - 0.943 g/cc
0.0339 - 0.0341 lb/in³
Kazanorgsintez PE80B-285SL High Density Polyethylene Composite, Film Grade
Production Method: Compositions are achieved by ethylene copolymerization by gaseous-phase method at low pressure using complex catalysts on carrier material. Application: HDPE compositions are ..
Density 0.927 - 0.944 g/cc
0.0335 - 0.0341 lb/in³
Requirement
Westlake Plastics Lennite® GUR1020 (Type I) Ultra-high Molecular Weight Polyethylene For Medical Applications
Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m..
Density 0.927 - 0.944 g/cc
0.0335 - 0.0341 lb/in³
Requirement
Westlake Plastics Lennite® GUR1050 (Type II) Ultra-high Molecular Weight Polyethylene For Medical Applications
Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m..
Density 0.916 - 0.944 g/cc
0.0331 - 0.0341 lb/in³
Average value: 0.922 g/cc Grade Count:20
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min..
Density 0.913 - 0.945 g/cc
0.0330 - 0.0341 lb/in³
Average value: 0.935 g/cc Grade Count:49
Overview of materials for Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Rotational Molding Grade". Each property range of values report..
Density 0.924 - 0.945 g/cc
0.0334 - 0.0341 lb/in³
Average value: 0.937 g/cc Grade Count:67
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i..
Density 0.927 - 0.945 g/cc
0.0335 - 0.0341 lb/in³
Average value: 0.939 g/cc Grade Count:17
Overview of materials for Ethylene-Methyl Acrylate Copolymer, Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene-Methyl Acrylate Copolymer, Molding Grade". Each property range of values reported is minimum an..