Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chevron Phillips Marlex® HHM TR-400G Medium density hexene copolymer  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chevron Phillips Marlex® HHM TR-400G Medium density hexene copolymer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Benefits: good processability, excellent melt strength, broad fusion range, outstanding stress cracking resistanceApplications: pond liners, gas and chemical tank containment liners, landfill linersInformation provided by Chevron Phillips Chemical Company
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1500 hour

@Temperature 50.0 °C
>= 1500 hour

@Temperature 122 °F
Condition B and Condition C; ASTM D 1693
High Load Melt Index 12 g/10 min

@Load 21.6 kg,
Temperature 190 °C
12 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
ASTM D638 Type IV
Elongation at Break >= 700 %
>= 700 %
ASTM D638 Type IV
Flexural Modulus 0.830 GPa
120 ksi
ASTM D790
Processing Properties Metric English Comments
Processing Temperature 193 - 210 °C
379 - 410 °F
stock temperature
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved