ExxonMobil Escorene™ UL 53019CC Ethylene Vinyl Acetate Copolymer (European Grade)

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Exxon Chemical
Trade Name Escorene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Escorene™ UL 53019CC Ethylene Vinyl Acetate Copolymer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: UL 53019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent: No Applications: Hot Melt Adhesives Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ExxonMobil method
Vinyl Acetate Content 19 %
19 %
ExxonMobil method
Melt Flow 530 g/10 min
530 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
Molded Properties; ASTM D2240
Tensile Strength at Break 3.17 MPa
460 psi
(20 in/min), Molded Properties; ASTM D638
Elongation at Break 230 %
230 %
(20 in/min), Molded Properties; ASTM D638
Tensile Modulus 0.0269 GPa
3.90 ksi
(0.2 in/min), Molded Properties; ASTM D638
Thermal Properties Metric English Comments
Melting Point <= 176 °C
<= 349 °F
Peak Melting Point; ExxonMobil method