Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Braskem LH 437 LMDPE Cast Film Extrusion Polyethylene  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem LH 437 LMDPE Cast Film Extrusion Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Diapers (back sheet); Absorbent pads (back sheet). Information provided by Braskem
Physical Properties Metric English Comments
Density 0.937 g/cc
0.0339 lb/in³
ASTM D1505
Melt Flow 4.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
ASTM D2240
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break >= 1000 %
>= 1000 %
ASTM D638
Flexural Modulus 0.804 GPa
117 ksi
ASTM D790
Secant Modulus 1.805 GPa
261.8 ksi
0.01; ASTM D638
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved