Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Noryl EN130 PPE+HIPS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Noryl EN130 PPE+HIPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
NORYL EN130 is an extrusion material with a Vicat B/120 of 140 deg C according ISO 306. NORYL EN130 is a standard extrusion grade for applications where higher temperature resistance is required. NORYL EN130 is available in all colours.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.070 %
0.070 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.25 %

@Temperature 23.0 °C
0.25 %

@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
on tensile bar; SABIC Method
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 100 MPa
14500 psi
ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
50 mm/min; ISO 527
Tensile Strength, Yield 50.0 MPa
7250 psi
50 mm/min; ISO 527
Elongation at Break 50 %
50 %
50 mm/min; ISO 527
Elongation at Yield 4.0 %
4.0 %
50 mm/min; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
Flexural Yield Strength 70.0 MPa
10200 psi
2 mm/min; ISO 178
Flexural Modulus 2.10 GPa
305 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
13.0 kJ/m²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 20

@Load 1.00 kg
20

@Load 2.20 lb
CS-17; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 60.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
33.3 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
38.9 µin/in-°F

@Temperature 73.4 - 176 °F
ISO 11359-2
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
ISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 135 °C
275 °F
Rate B/50; ISO 306
140 °C
284 °F
Rate B/120; ISO 306
145 °C
293 °F
Rate A/50; ISO 306
Flammability, UL94 HB

@Thickness 1.65 mm
HB

@Thickness 0.0650 in
UL 94 by SABIC-IP
Oxygen Index 24 %
24 %
LOI; ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
IEC 60250
2.7

@Frequency 50.0 - 60.0 Hz
2.7

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 22.0 kV/mm

@Thickness 3.20 mm
559 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor 0.00090

@Frequency 1.00e+6 Hz
0.00090

@Frequency 1.00e+6 Hz
IEC 60250
0.0040

@Frequency 50.0 - 60.0 Hz
0.0040

@Frequency 50.0 - 60.0 Hz
IEC 60250
Descriptive Properties Value Comments
Ball Pressure Test, 125°C +/- 2°C PASSES
IEC 60695-10-2