| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP ..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® EFX810ME PC
Modified PC blend offering metallic / sparkle look with minimal flowline visibility.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® EFX810ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flowline visibility.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Thickness 4.00 mm,<br> Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Thickness 0.157 in,<br> Temperature -22.0 °F
|
ISO 180/1A |
|
Polimeri Europa Edistir ICE S 800/N Polystyrene
(discontinued **)
Very high environmental stress cracking resistant (VH ESCR) modified HIPS. ICE S 800/N exhibits high toughness and excellent chemical resistance to oils, fats and chemical agents and in particular t..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® DMX1214 PC Copolymer
Lexan* DMX1214 resin is an improved flow, transparent copolycarbonate resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -40.0 °C
|
2.86
ft-lb/in² <br>@Temperature -40.0 °F
|
50%RH; ISO 180/1A |
|
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem 1000FV PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem HU1000E PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East)
Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem ATX152R PEI+PCE
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -40.0 °C
|
2.86
ft-lb/in² <br>@Temperature -40.0 °F
|
80x10x4; ISO 180/1A |
|
Eurostar Staramide AG3X3 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding
Staramide AG3X3 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecodur® PB70 CR30 BK111 PBT, 30% carbon fiber reinforced, black
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecodur® PB70 GR15 NL XA 20 PBT 15% glass fiber reinforced, UL94 V0
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecodur® PB70 GR23 BK EF PBT, 23% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA30 NL RM PA6.6, MoS2 modified, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
80x10x4; ISO 180/1A |
|
Eurostar Starflam AFR450B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding
Starflam AFR450B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA40 GR15 NL PA 6.6 15% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature 23.0 °C
|
2.86
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, Conditioned
Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® 66B Nylon 66, General Purpose, high viscosity, Conditioned
Vydyne® 66B is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66B resin offers high strength, ..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -20.0 °C
|
2.86
ft-lb/in² <br>@Temperature -4.00 °F
|
ISO 180 |
|
Total PPC 3120 MU5 Polypropylene, Heterophasic Copolymer, Automotive
Polypropylene PPC 3120 MU5 is a heterophasic copolymer with a Melt Flow index of 15 g/10 min. Polypropylene PPC 3120 MU5 is a high impact copolymer formulated to give good UV resistance.Polypropyle..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**)
Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NB40 NL FY50 PA6, unfilled, flame retardant - halogen & red phosphorus free, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® 67R Nylon 66, Heat Stabilized, DAM
Vydyne® 67R is a high-viscosity, heat-stabilized PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 67R resin offers high strength, ..
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® ML3286 PC (Europe-Africa-Middle East)
LEXAN ML3286 is a 17% glass reinforced grade for use in less demanding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
6.00
kJ/m² <br>@Temperature -30.0 °C
|
2.86
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, Conditioned
Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced ..
|
|||