PSM Industries PM Krupp M-2 Powder Metallurgy Steel Alloy

Category Metal , Ferrous Metal , Alloy Steel , Tool Steel
Manufacturer PSM Industries
Trade Name PM Krupp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PSM Industries PM Krupp M-2 Powder Metallurgy Steel Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PSM Industries is a company that is using Powder Metallurgy technologies to create engineered materials for applications requiring extreme wear resistance and toughness. The drive is to use conventional Powder Metallurgy tooling to capture net or near net shapes in materials that were previously were ingot-cast wrought products. By capturing more net shape, the result is that the number of costly secondary labor operations are reduced which translates to lower manufacturing costs.Information Provided by PM Krupp, a division of PSM Industries
Mechanical Properties Metric English Comments
Hardness, Rockwell C 62 - 64
62 - 64
Component Elements Properties Metric English Comments
Carbon, C 0.78 - 0.88 %
0.78 - 0.88 %
Chromium, Cr 3.75 - 4.5 %
3.75 - 4.5 %
Manganese, Mn 0.15 - 0.40 %
0.15 - 0.40 %
Molybdenum, Mo 4.5 - 5.5 %
4.5 - 5.5 %
Phosphorous, P <= 0.030 %
<= 0.030 %
Silicon, Si 0.20 - 0.45 %
0.20 - 0.45 %
Sulfur, S <= 0.030 %
<= 0.030 %
Tungsten, W 5.5 - 6.75 %
5.5 - 6.75 %
Vanadium, V 1.75 - 2.2 %
1.75 - 2.2 %