| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Noryl |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.11 g/cc | 1.11 g/cc | ASTM D792 |
| Density | 1.11 g/cc | 0.0401 lb/in³ | ISO 1183 |
| Water Absorption at Saturation | 0.060 % | 0.060 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 25 g/10 min @Load 5.00 kg, Temperature 250 °C |
25 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
| Melt Index of Compound | 25 g/10 min @Load 2.16 kg, Temperature 280 °C |
25 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 46.0 MPa | 6670 psi | 50 mm/min; ISO 527 |
| 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 58.0 MPa | 8410 psi | 50 mm/min; ISO 527 |
| 67.0 MPa | 9720 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | 4.4 % | 4.4 % | 50 mm/min; ISO 527 |
| 5.2 % | 5.2 % | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Yield | 3.3 % | 3.3 % | 50 mm/min; ISO 527 |
| 3.6 % | 3.6 % | Type I, 50 mm/min; ASTM D638 | |
| Tensile Modulus | 2.50 GPa | 363 ksi | 1 mm/min; ISO 527 |
| 2.56 GPa | 371 ksi | 5 mm/min; ASTM D638 | |
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
| 100 MPa | 14500 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.50 GPa | 363 ksi | 2 mm/min; ISO 178 |
| 2.73 GPa | 396 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
| 0.200 J/cm @Temperature -30.0 °C |
0.375 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² | 3.81 ft-lb/in² | 80*10*4; ISO 180/1A |
| 4.00 kJ/m² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.00 J/cm² | 4.76 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 30.0 J @Temperature 23.0 °C |
22.1 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 77.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 77.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
42.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
| 79.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
43.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 75.0 °C | 167 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 75.0 °C @Thickness 3.20 mm |
167 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
| 83.0 °C @Thickness 6.40 mm |
181 °F @Thickness 0.252 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 96.0 °C | 205 °F | Rate B/50; ASTM D1525 |
| 96.0 °C | 205 °F | Rate B/50; ISO 306 | |
| 98.0 °C | 208 °F | Rate B/120; ISO 306 | |
| Flammability, UL94 | V-1 @Thickness 1.50 mm |
V-1 @Thickness 0.0591 in |
UL 94 by SABIC-IP |
| V-0 @Thickness 2.50 mm |
V-0 @Thickness 0.0984 in |
UL 94 by SABIC-IP |