| Category | Metal , Nonferrous Metal , Nickel Alloy , Superalloy |
| Manufacturer | High Performance Alloys, Inc |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 9.22 g/cc | 0.333 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Brinell | 415 | 415 | Estimated from Rockwell C |
| Hardness, Rockwell A | 73 | 73 | Estimated from Rockwell C |
| Hardness, Rockwell C | 45 | 45 | |
| Hardness, Vickers | 440 | 440 | Estimated from Rockwell C |
| Modulus of Elasticity | 189 GPa @Thickness 12.7 mm, Temperature 538 °C |
27400 ksi @Thickness 0.500 in, Temperature 1000 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
| 196 GPa @Thickness 12.7 mm, Temperature 427 °C |
28400 ksi @Thickness 0.500 in, Temperature 800 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) | |
| 202 GPa @Thickness 12.7 mm, Temperature 316 °C |
29300 ksi @Thickness 0.500 in, Temperature 600 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) | |
| 217 GPa @Thickness 12.7 mm, Temperature 21.1 °C |
31500 ksi @Thickness 0.500 in, Temperature 70.0 °F |
(Heat treated at 1066°C (1950°F), rapid quenched, plate) |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 93.0 °C |
5.72 µin/in-°F @Temperature 68.0 - 199 °F |
|
| 10.8 µm/m-°C @Temperature 20.0 - 204 °C |
6.00 µin/in-°F @Temperature 68.0 - 399 °F |
||
| 11.2 µm/m-°C @Temperature 20.0 - 316 °C |
6.22 µin/in-°F @Temperature 68.0 - 601 °F |
||
| 11.5 µm/m-°C @Temperature 20.0 - 427 °C |
6.39 µin/in-°F @Temperature 68.0 - 801 °F |
||
| 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
||
| Specific Heat Capacity | 0.373 J/g-°C @Temperature 0.000 °C |
0.0891 BTU/lb-°F @Temperature 32.0 °F |
|
| 0.389 J/g-°C @Temperature 100 °C |
0.0930 BTU/lb-°F @Temperature 212 °F |
||
| 0.406 J/g-°C @Temperature 200 °C |
0.0970 BTU/lb-°F @Temperature 392 °F |
||
| 0.423 J/g-°C @Temperature 300 °C |
0.101 BTU/lb-°F @Temperature 572 °F |
||
| 0.431 J/g-°C @Temperature 400 °C |
0.103 BTU/lb-°F @Temperature 752 °F |
||
| 0.444 J/g-°C @Temperature 500 °C |
0.106 BTU/lb-°F @Temperature 932 °F |
||
| 0.456 J/g-°C @Temperature 600 °C |
0.109 BTU/lb-°F @Temperature 1110 °F |
||
| Thermal Conductivity | 11.1 W/m-K @Temperature 0.000 °C |
77.0 BTU-in/hr-ft²-°F @Temperature 32.0 °F |
|
| 12.2 W/m-K @Temperature 100 °C |
84.7 BTU-in/hr-ft²-°F @Temperature 212 °F |
||
| 13.4 W/m-K @Temperature 200 °C |
93.0 BTU-in/hr-ft²-°F @Temperature 392 °F |
||
| 14.6 W/m-K @Temperature 300 °C |
101 BTU-in/hr-ft²-°F @Temperature 572 °F |
||
| 16.0 W/m-K @Temperature 400 °C |
111 BTU-in/hr-ft²-°F @Temperature 752 °F |
||
| 17.3 W/m-K @Temperature 500 °C |
120 BTU-in/hr-ft²-°F @Temperature 932 °F |
||
| 18.7 W/m-K @Temperature 600 °C |
130 BTU-in/hr-ft²-°F @Temperature 1110 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | 0.010 % | 0.010 % | |
| Chromium, Cr | 1.0 % | 1.0 % | |
| Cobalt, Co | <= 1.0 % | <= 1.0 % | |
| Iron, Fe | <= 2.0 % | <= 2.0 % | |
| Manganese, Mn | <= 1.0 % | <= 1.0 % | |
| Molybdenum, Mo | 28 % | 28 % | |
| Nickel, Ni | 69 % | 69 % | |
| Silicon, Si | <= 0.10 % | <= 0.10 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.000137 ohm-cm @Temperature 0.000 °C |
0.000137 ohm-cm @Temperature 32.0 °F |
|
| 0.000138 ohm-cm @Temperature 100 °C |
0.000138 ohm-cm @Temperature 212 °F |
||
| 0.000138 ohm-cm @Temperature 200 °C |
0.000138 ohm-cm @Temperature 392 °F |
||
| 0.000139 ohm-cm @Temperature 300 °C |
0.000139 ohm-cm @Temperature 572 °F |
||
| 0.000139 ohm-cm @Temperature 400 °C |
0.000139 ohm-cm @Temperature 752 °F |
||
| 0.000141 ohm-cm @Temperature 500 °C |
0.000141 ohm-cm @Temperature 932 °F |
||
| 0.000146 ohm-cm @Temperature 600 °C |
0.000146 ohm-cm @Temperature 1110 °F |