| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycoloy® C1000 PC+ABS (Europe-Africa-Middle East)
CYCOLOY C1000 is a PC+ABS blend developed with emphasis on excellent processing efficiency while maintaining good heat resistance and impact ductility. It is an excellent material choice for a wide ..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East)
Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycoloy® CU6800 PC+ABS (Europe-Africa-Middle East)
Non-chlorinated and non-brominated flame retardant PC/ABS featuring excellent flow properties for a wide variety of applications including business equipment, TVs, monitors, enclosures, among others..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | ISO 178, ASTM D790 |
|
Nilit Nilitop BT N Unfilled, Nucleated PBT
Description: Nilitop BT N is an unfilled, nucleated PBT that has excellent cycle times.Key characteristics: Good overall mechanical performanceLow moisture absorptionExcellent UV resistanceExcellent..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycoloy® CY4000 PC+ABS (Europe-Africa-Middle East)
Cycoloy* CY4000 resin is an injection moldable, flame retardant PC/ABS blend free of brominated or chlorinated flame resistant additives. Cycoloy CY4000 has excellent flow and balanced impact proper..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Cycoloy® HCX1640 PC+ABS (Europe-Africa-Middle East)
CYCOLOY™ HCX1640 a PC+ABS blend specially developed for medical devices and pharmaceutical applications requiring improved mechanical performance . It combines good flow with excellent impact and l..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS (Asia Pacific)
IP1000 is a high impact PC/ABS blend developed for the automotive instrument panel business.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS
Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® 943X PC Copolymer
Lexan* 943X is a UV stabilized medium flow impact modified injection molding (IM) grade. This resin offers UL94 V0 @ 1.5mm flame retardancy based on non-bromine, non-chlorine FR systems, low tempera..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® EXL1444 PC Copolymer
Lexan* EXL1444 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade suitable for FDA compliant applications. This resin offers extreme low temperature (-..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific)
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® FXG1413T PC Copolymer (Asia Pacific)
PC-siloxane copolymer in special ""Diamond Sparkle"" colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Lexan® FXM1414T PC Copolymer (Europe-Africa-Middle East)
PC-siloxane copolymer in special metallic colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.This data was supplied by ..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® FXM3729 PC (Europe-Africa-Middle East)
LEXAN FXM3729 is an UV stabilized Visual FX Sparkle grade, with an excellent flow. It contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Midd..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® HP1HF PC
Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® ML7652 PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. Medium flow, excellent low temperature ductility.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Geloy XTPM309E ASA+PC (Europe-Africa-Middle East)
XTPM309E is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour stab..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® EXL1414 PC Copolymer (Europe-Africa-Middle East)
Lexan* EXL1414 polycarbonate (PC) siloxane copolymer resin is a medium flow opaque injection molding (IM) grade. This resin offers extreme low temperature (-40 C) ductility in combination with excel..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® FXD1414T PC Copolymer
PC-siloxane copolymer in special light diffusion colors. Medium flow. Improved toughness compared to medium flow standard PC in same color. Color package may affect performance.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | ASTM D790 |
|
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose
(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® VX3101N PBT (Europe-Africa-Middle East)
VALOX VX3101N is an unreinforced PBT injection moulding resin, with excellent flow properties, good hydrolitical stability and chemical resistance.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East)
Low-medium flow, suitable for blow molding, injection molding, extrusion.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Europe-Africa-Middle East)
high gloss Noryl
|
|||
| Flexural Yield Strength | >= 85.0 MPa | >= 12300 psi | ASTM D790 |
|
Cresset Powers Cress-Alon™ A2700 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded
Neat resin, for compounding.Information provided by Cresset Powers Ltd.
|
|||
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
|
|||
| Flexural Yield Strength |
85.0
-
275
MPa <br>@Temperature -40.0 - 120 °C
|
12300
-
39900
psi <br>@Temperature -40.0 - 248 °F
|
Average value: 180 MPa Grade Count:1 |
|
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..
|
|||