Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resinoid 1363 Phenolic Molding, Glass Reinforced

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Resinoid
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resinoid 1363 Phenolic Molding, Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
Physical Properties Metric English Comments
Density 1.75 g/cc
0.0632 lb/in³
ASTM D792A
Water Absorption 0.10 %
0.10 %
24 hours R.T. ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ASTM D651
Flexural Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 18.0 GPa
2610 ksi
ASTM D790
Compressive Strength 234 MPa
33900 psi
ASTM D695
Izod Impact, Notched 1.58 J/cm
2.96 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 300 °C
>= 572 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 13.0 kV/mm
330 kV/in
Short Time; Dry; ASTM D149
Processing Properties Metric English Comments
Mold Temperature 155 - 180 °C
311 - 356 °F