| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® EXL1434 PC Copolymer (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
| Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.150 % | 0.150 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.35 % | 0.35 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm <br>@Thickness 3.20 mm |
0.0040 - 0.0080 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm <br>@Thickness 3.20 mm |
0.0040 - 0.0080 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 10 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
10 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 9.0 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
9.0 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell L | 89 | 89 | ASTM D785 |
| Hardness, Rockwell R | 121 | 121 | ASTM D785 |
| Tensile Strength at Break | 50.0 MPa | 7250 psi | Type I, 50 mm/min; ASTM D638 |
| 60.0 MPa | 8700 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 55.0 MPa | 7980 psi | Type I, 50 mm/min; ASTM D638 |
| 57.0 MPa | 8270 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 98 % | 98 % | Type I, 50 mm/min; ASTM D638 |
| 120 % | 120 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 6.0 % | 6.0 % | Type I, 50 mm/min; ASTM D638 |
| 6.0 % | 6.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.02 GPa | 293 ksi | 50 mm/min; ASTM D638 |
| 2.15 GPa | 312 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 85.0 MPa | 12300 psi | 2 mm/min; ISO 178 |
| 92.0 MPa | 13300 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.23 GPa | 323 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 2.25 GPa | 326 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 8.65 J/cm | 16.2 ft-lb/in | ASTM D256 |
| 7.74 J/cm <br>@Temperature -30.0 °C |
14.5 ft-lb/in <br>@Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² | 80*10*3; ISO 180/1A |
| 60.0 kJ/m² <br>@Temperature -30.0 °C |
28.6 ft-lb/in² <br>@Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
| NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
| Charpy Impact Unnotched | NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
| NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
| Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 6.50 J/cm² <br>@Temperature -30.0 °C |
30.9 ft-lb/in² <br>@Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 70.0 J <br>@Temperature 23.0 °C |
51.6 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 69.7 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
38.7 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 72.0 µm/m-°C <br>@Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F <br>@Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 72.0 µm/m-°C <br>@Temperature 23.0 - 80.0 °C |
40.0 µin/in-°F <br>@Temperature 73.4 - 176 °F |
ISO 11359-2 |
| 74.7 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
41.5 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 140 °C | 284 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
| 139 °C <br>@Thickness 3.20 mm |
282 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 128 °C | 262 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 124 °C <br>@Thickness 3.20 mm |
255 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 145 °C | 293 °F | Rate B/50; ASTM D1525 |
| 145 °C | 293 °F | Rate B/50; ISO 306 | |
| 146 °C | 295 °F | Rate B/120; ISO 306 | |
| UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
| UL RTI, Mechanical with Impact | 120 °C | 248 °F | UL 746B |
| UL RTI, Mechanical without Impact | 125 °C | 257 °F | UL 746B |
| Oxygen Index | 37 % | 37 % | ISO 4589 |
| Glow Wire Test | 875 °C | 1610 °F | IEC 60695-2-13 |
| 875 °C | 1610 °F | IEC 60695-2-13 | |
| 850 °C <br>@Thickness 0.800 mm |
1560 °F <br>@Thickness 0.0315 in |
IEC 60695-2-12 | |
| 960 °C <br>@Thickness 1.00 mm |
1760 °F <br>@Thickness 0.0394 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | ASTM D257 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ASTM D257 |
| Dielectric Constant | 2.64 <br>@Frequency 1.00e+6 Hz |
2.64 <br>@Frequency 1.00e+6 Hz |
ASTM D150 |
| 2.68 <br>@Frequency 100 Hz |
2.68 <br>@Frequency 100 Hz |
ASTM D150 | |
| Dielectric Strength | 16.2 kV/mm <br>@Thickness 0.800 mm |
411 kV/in <br>@Thickness 0.0315 in |
in oil; ASTM D149 |
| Dissipation Factor | 0.0012 <br>@Frequency 100 Hz |
0.0012 <br>@Frequency 100 Hz |
ASTM D150 |
| 0.0093 <br>@Frequency 1.00e+6 Hz |
0.0093 <br>@Frequency 1.00e+6 Hz |
ASTM D150 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | Passes | IEC 60695-10-2 |