Polymer Property : Vicat Softening Point = 226 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 108 °C
226 °F
ASTM D-1525
Plaskolite Optix® CP - 927 GHF High Impact Grade Acrylic Resin
OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc.
Vicat Softening Point 108 °C
226 °F
Rate A, ASTM D1525
Plaskolite West Optix® CA-927 HF Clear Impact Modified Acrylic Resin
Impact modified acrylic resin, injection molding gradeApplications: A high flow, impact-modified acrylic resin for injection molding. This resin offers impact strengths up to seven times those of g..
Vicat Softening Point 108 °C
226 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS
Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal ..
Vicat Softening Point 108 °C
226 °F
Rate B/50; ISO 306
SABIC Innovative Plastics GELOY FXW751SK ASA+PC (Asia Pacific)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin
Vicat Softening Point 108 °C
226 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East)
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 108 °C
226 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Lexan® ML7686E PC (Europe-Africa-Middle East)
Transparent Polycarbonate in natural color. Excellent processability, super high flow. UL compliant 94V-2 at 1.5mm.
Vicat Softening Point 108 °C
226 °F
Americas Styrenics Styron® 663 Polystyrene  (discontinued **)
STYRON® 663 general purpose polystyrene resin is an additive free resin with excellent strength, clarity, and high heat resistance. When used unmodified for the manufacture of food contact articles..
Vicat Softening Point 108 °C
226 °F
ASTM D1525
Eastman E6837-539A Polyethylene  (discontinued **)
PolyethyleneE6837-539A is used in various injection molding applications including closures for containers or extrusion coating for high stiffness. It has good processability. This product may be us..
Vicat Softening Point 108 °C
226 °F
ASTM D1525
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 31% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro..
Vicat Softening Point 108 °C

@Load 1.00 kg,
Thickness 3.17 mm
226 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
IRPC Polimaxx Polene 320PC Styrene Acrylonitrile
APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN
Vicat Softening Point 108 °C

@Load 1.00 kg,
Thickness 3.17 mm
226 °F

@Load 2.20 lb,
Thickness 0.125 in
ASTM D1525
IRPC Polimaxx Polene 330PC Styrene Acrylonitrile
APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN
Vicat Softening Point 108 °C
226 °F
ISO 306A
Lucite International Diakon® CLG902LX Acrylic Polymer
Information provided by Lucite International
Vicat Softening Point 108 °C
226 °F
ISO 306B
Lucite International Diakon® CMH454 Acrylic Polymer
Information provided by Lucite International
Vicat Softening Point 108 °C
226 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
Vicat Softening Point 108 °C
226 °F
B/50; ISO R306
Samsung Cheil Industries Infino® UF-1013 PC, Unreinforced FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 108 °C
226 °F
B/120; ISO R306
Samsung Cheil Industries Starex® GR-4010 ABS, 10% Glass Filled
Material with 10% GF reinforcement with high stiffness that can be used in refrigerator vegetable boxesInformation provided by Samsung Cheil Industries.
Vicat Softening Point 108 °C
226 °F
VST/A/120; ISO 306
Styrolution Polystyrol 168 N GR 2 PS
Description: Polystyrol 168 N is a high molecular, heat grade used where high strength is required. Suitable for physically or chemically expanded extruded sheet. As blend component with high impact..
Vicat Softening Point 108 °C
226 °F
B/50; ISO R306
Samsung Cheil Industries Starex® WR-9370 ASA, Unreinforced Heat Resistant
Information provided by Samsung Cheil Industries.
Vicat Softening Point 108 °C
226 °F
Styron Magnumâ„¢ 2610 ABS, High Gloss
MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM ..
Vicat Softening Point 108 °C
226 °F
ASTM D1525
Styron MAGNUMâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3325 MT is a resin with excellent processing characteristics and matt surface finish. The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines..
Vicat Softening Point 108 °C
226 °F
ASTM D1525
PlastxWorld CEVIAN® VGR10 10% GF ABS
Glass fiber reinforced ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Vicat Softening Point 108 °C
226 °F
A (10N); ISO 306
Borealis Borstar® FB2310 LLDPE for Film
Borstar BF2310 is a high molecular weight low density polyethylene film grade combining good and flexible extrusion behavior, excellent draw down and superior mechanical properties. Film made from ..
Vicat Softening Point 108 °C
226 °F
Rate B; ISO 306
Covestro Bayblend® 2953 Polycarbonate + ABS Blend, Automotive Plating
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Vicat Softening Point 108 °C
226 °F
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend
Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, good light stability.Applications: Housings for business machines.Information provided by Bayer.As of 1 Septe..
Vicat Softening Point 108 °C
226 °F
50°C/h 50N; ISO 306
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (..
Vicat Softening Point 108 °C

@Thickness 6.35 mm
226 °F

@Thickness 0.250 in
Rate B; ASTM D-1525
Chevron Phillips MB3150 Crystal Polystyrene
High heat crystal polystyrene.Applications:Compact disc jewel boxesConsumer containers, vials, jars, etc.Desk organizersAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat sof..
Vicat Softening Point 108 °C
226 °F
ASTM D1525
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
DOWLEX™ 2045G resin is designed for the production of a wide variety of industrial and consumer films (though it is not recommended for silage stretch film). The product also delivers very good pr..
Vicat Softening Point 108 °C
226 °F
Method B; ASTM D-1525
Bhansali Engineering Abstron HR-60 ABS Heat Resistant
High, Medium Impact Heat Resistant Grades with good flowInformation provided by Bhansali
Vicat Softening Point 108 °C
226 °F
Rate B/50; ISO 306
SABIC Innovative Plastics GELOY FXW751SK ASA+PC
Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact Resin