Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Plastcom SLOVAMID 6 FRC 2 LI PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Pyrotek Pyroslip 105 RFU High-Purity Graphite-Based Lubricant Thick fluid consistency.ApplicationsSeamless steel pipe mandrel bar lubricant Aluminum extrusions billet and/or dummy block lubricant Hot steel closes die forging AdvantagesEnvironmentally friendly .. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Geloy FXW751SK ASA+PC (Europe-Africa-Middle East) Sparkle Metallic VisualFx ASA+PC Resin - Weatherable, High Heat & Impact ResinThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Noltex Soarnol® ET3803 Ethylene Vinyl Alcohol Copolymer Medium ethylene content. Suitable for packaging a wet product in a wet environment. Preferred for use in forming webs for meat and cheese packaging. Ethylene content 38 mol%. Volatile matter 0.3%... |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
Lucite International Diakon® TD735 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Density | 1.16 - 1.22 g/cc | 0.0419 - 0.0441 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 6221 C GREY The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | DIN 53479; ASTM D792 |
Kolon KOPA® KN132VO Flame Retardant Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | |
Taiwan Sheen Soon Sheenthane® A8521H TPU for Ink Thermoplastic polyurethane elastomer for ink. Hydrolysis resistance gradeAbrasion resistant, flexible, soft, excellent adhesion, high solubility in MEK and Anone. Used for transfer coating, screen.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Lubricomp QP003 PA 6/10 (Asia Pacific) LNP* Lubricomp* QP003 is a compound based on Nylon 6/10 resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the As.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO R 1183 |
Schwartz Technical Plastics LAMIGAMID® 324 Cast Polyamide 6, MoS2, Heat Stabilized, Dry Application: heavy-duty wheels, running speed up to 3m/sInformation provided by Schwartz Technical Plastics GmbH |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RN001S PA 66 LNP* LUBRICOMP* RN001S is a compound based on Nylon 66 resin containing 2% MOS2. Added features of this material include: Wear Resistant, Heat Stabilized. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Techmer ES HiFill® ABS GB15 15% Glass Bead Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Stellarchem MP-835B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
SABIC Innovative Plastics XYLEX X8210 PC+POLYESTER PC+POLYESTER alloy. Unreinforced, transparent, impact modified for low temperature ductility |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Loctite® 392 Rapid Fixture Structural Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Density | 1.16 g/cc @Temperature 270 °C |
0.0419 lb/in³ @Temperature 518 °F |
Melt |
Covestro Makroblend® DP 7665 Polycarbonate + PET, Mineral Filled Impact Grade Developmental productISO 7792-1-PC/PET,MHPR,-030,MD20(PC+PET)-blendsimpact modifiedInjection molding grade 20 % mineral filledPreprocessingMax. Water content |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
DSM Arnitel® EM460 46 Shore D, Injection Molding or Extrusion Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ISO 1183 |
DSM Arnitel® VT3104 TPC-ET Extrusion Grade |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
DSM Somos® GP Plus 14122 Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually .. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
Epoxyset Epoxibond EB-130M-1 Unfilled Epoxy Adhesive A two-component, non-hazmat, unfilled epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | ASTM D792 |
Engineered Plastics EP Alloy 510G PC/ABS Alloy Black. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Proper.. |
|||
Density | 1.16 - 1.20 g/cc | 0.0419 - 0.0434 lb/in³ | ISO R 1183 |
Fainplast Compounds PM 55 Flexible PVC, Lead Free Gaskets for frames |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 19540R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 1523 Style FiberglassThis data represents typical values for the production material. The data should not be u.. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
A. Schulman ComAlloy Comshield® 229 ABS, Electrically Conductive - Stainless Steel Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.16 g/cc | 0.0419 lb/in³ | |
A. Schulman ComAlloy Hiloy® 123 Polypropylene, Glass Reinforced, Chemically Coupled, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.16 - 1.31 g/cc | 0.0419 - 0.0473 lb/in³ | Average value: 1.19 g/cc Grade Count:92 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |