| Category | Polymer , Thermoplastic , ASA Polymer |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | GELOY |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics GELOY CR7500 ASA.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
| Moisture Absorption | 0.200 % | 0.200 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.50 % | 0.50 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0080 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0080 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 6.3 g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C |
6.3 g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F |
ASTM D1238 |
| 11 g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C |
11 g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F |
ASTM D1238 | |
| Melt Index of Compound | 6.0 g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C |
6.0 g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
| 10 g/10 min <br>@Load 5.00 kg,<br> Temperature 260 °C |
10 g/10 min <br>@Load 11.0 lb,<br> Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 33.0 MPa | 4790 psi | Type I, 5 mm/min; ASTM D638 |
| 35.0 MPa | 5080 psi | 5 mm/min; ISO 527 | |
| Tensile Strength, Yield | 40.0 MPa | 5800 psi | Type I, 5 mm/min; ASTM D638 |
| 43.0 MPa | 6240 psi | 5 mm/min; ISO 527 | |
| Elongation at Break | 19 % | 19 % | 5 mm/min; ISO 527 |
| 60 % | 60 % | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Yield | 3.3 % | 3.3 % | 5 mm/min; ISO 527 |
| 3.6 % | 3.6 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 1.97 GPa | 286 ksi | 5 mm/min; ASTM D638 |
| 2.04 GPa | 296 ksi | 1 mm/min; ISO 527 | |
| Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
| 68.0 MPa | 9860 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.06 GPa | 299 ksi | 2 mm/min; ISO 178 |
| 2.17 GPa | 315 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 4.00 J/cm | 7.49 ft-lb/in | ASTM D256 |
| 0.600 J/cm <br>@Temperature -30.0 °C |
1.12 ft-lb/in <br>@Temperature -22.0 °F |
ASTM D256 | |
| Izod Impact, Notched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1A |
| 6.00 kJ/m² <br>@Temperature -30.0 °C |
2.86 ft-lb/in² <br>@Temperature -22.0 °F |
80*10*4; ISO 180/1A | |
| Charpy Impact, Notched | 1.40 J/cm² | 6.66 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
| Dart Drop, Total Energy | 30.0 J <br>@Temperature 23.0 °C |
22.1 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 84.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
46.7 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 84.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
46.7 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 95.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 |
| 95.0 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ISO 11359-2 | |
| Hot Ball Pressure Test | <= 98.0 °C | <= 208 °F | IEC 60695-10-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 88.0 °C | 190 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
| 89.0 °C | 192 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af | |
| 90.0 °C <br>@Thickness 3.20 mm |
194 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 98.0 °C | 208 °F | Rate B/50; ASTM D1525 |
| 102 °C | 216 °F | Rate B/50; ISO 306 | |
| 105 °C | 221 °F | Rate B/120; ISO 306 |