Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 90.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
annealed; ASTM D648
Plaskolite Duraplex® 50% I Impact Modified Acrylic Sheet
Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
STN EN ISO 75/A
Plastcom SLOVALEN PC 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc
FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C...
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
120°C/h; ISO 75/1
Polykemi AB POLYblend 45V PC/ABS-blend, Flame Retardant
Information provided by Polykemi AB
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
120°C/h; ISO 75/1
Polykemi AB POLYfill PP CIM9040 Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
<br>@Thickness 3.20 mm
194 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CM6210 PC+ABS
Cycoloy* resin CM6210 is a high-modulus flame retardant PC/ABS with non-brominated and non-chlorinated FR system. It can be used for extrusion & thermoforming applications and also for injection mol..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
120°C/h; ISO 75/1
Polykemi AB POLYabs HH0 ABS, Extra Heat Resistance
Information provided by Polykemi AB
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
LATI Lastilac MR MDT05-01 ABS
Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Magnetic detectable filler. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North ..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
<br>@Thickness 3.20 mm
194 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP LUBRICOMP KL005 Acetal Copolymer (Asia Pacific)
LNP* LUBRICOMP* KL005 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER
PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific)
LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75
Styrolution PS 156F GPPS
Styrolution PS 156F is a general purpose polystyrene grade with excellent flow properties, high heat resistance and is zinc stearate free.Free of internal lubricantsHigh heat resistanceExcellent flo..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
<br>@Thickness 3.20 mm
194 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
0.25 inch; ASTM D648
PlastxWorld CEVIAN® B1500 PBT/ABS Alloy
Unfilled, Excellent ToughnessThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
0.5 inch; ASTM D648
PlastxWorld CEVIAN®-N 055 SAN resin
These are typical values and are not intended for specification purposes. UL approved file No. is E142893. Information provided by PlastxWorld Inc.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
@ 264 psi; ASTM D648
Videolar 825 High Impact Polystyrene (HIPS)
Injection molding gradeMedium melt flow and high glossGood balance between rigidity and impactFeatures: Excellent mechanical strengthExcellent temperature resistancehigh impactApplications: Toys, ap..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
A. Schulman VOLOY™ 461 Glass Reinforced, Flame Retardant PBT Alloy
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
A. Schulman SCHULAMID® 66 MK20HI 20% Mineral Reinforced, Impact Modified Nylon 66
Information provided by A. Schulman.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/-2
Covestro Bayblend® FR 3010 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradeincreased heat resistanceVicat/B 120 temperature = 110 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantglow wire test (GWFI): 960 °C (..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1,-2
Covestro Bayblend® FR3010 HF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
Diamond Polymers NYLON 66 Natural
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-1/-2
EMS-Grivory Grivory® TR 90 TL PAMACM12
Product description: Grilamid TR 90 TL is a transparent thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic blocks. The special characteristic of Grilamid TR 90 TL is the high st..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Unannealed; ISO 75-2/A
Ascend Performance Materials Vydyne® 20NSP BLK Nylon 66, DAM
Vydyne® 20NSP BLK is a general-purpose, high nucleated, lubricated PA66 resin. Available in black, it is designed to crystallize rapidly in order to reduce cycle times and increase productivity thr..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced
High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
Supreme Petrochem SP 8001 High Gloss, ESCR High Impact Polystyrene
Characteristics Very high toughness Excellent ESCR properties against common food chemicals High gloss & heat resistance Processing Extrusion & Forming Applications Fatty food containers Co-extru..
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
<br>@Thickness 3.20 mm
194 °F
<br>@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Asia Pacific)
Cycoloy Medium Heat Plating Grade for Automotive
Copyright © lookpolymers.com All Rights Reserved