Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 64.0 MPa | 9280 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycolac® MG29 ABS Super high impact ABS. Good low temperature toughness. High gloss. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY CR8510 ASA ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy XTWM206 ASA (Europe-Africa-Middle East) Next generation ASA optimized for outstanding weatherability, colorability and higher heat applications requiring UV exposure resistance.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Rotuba H4 Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Asia Pacific) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Asia Pacific region... |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Geloy FXTW26SK ASA (Europe-Africa-Middle East) Next generation Geloy XTW ASA for high heat exterior applications. Outstanding weatherability and toughness. Metallic sparkle VisualFx.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Kleerdex Kydex® P54 Acrylic/PVC Extrusion Compound
(discontinued **) High impact profile extrusion compoundApplications: Extruded profiles requiring high impact, good chemical resistance, weatherability, and excellent flammability resistance.Features: P54 is extremel.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
KYDEX® 100 Acrylic/PVC Thermoplastic Sheet High impact fire rated sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones. Hidden parts for equipment such as vending machines.. |
|||
Flexural Yield Strength | 64.0 MPa @Thickness 6.40 mm |
9280 psi @Thickness 0.252 in |
ASTM D 790 |
SABIC Innovative Plastics Prevex BJAX PPE+PS Foamable resin. All properties at 10% density reduction; 0.250" thick specimens; improved productivity.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp ZP003 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZP003 is a compound based on PPE + PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC (Asia Pacific) Impact modified, highly chemical resistant polyester/polycarbonate alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Asia Pacific) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL PVX524 PPE PREVEX* PVX524 resin is a high flow, non FR grade, 100 C HDT |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific) PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Eastman Tritan LX150HF Copolyester Eastman Tritan LX150HF is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Eastman Tritan LX150HF has viscosity reductions of 40-50% relative to standard grades .. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Eastman Tritan MX730 Copolyester Eastman Tritan Copolyester MX730 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX730 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Eastman Tritan MX731 Copolyester Eastman Tritan Copolyester MX731 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX731 is a high flow medical grade of Eastman Tritan that has viscosity re.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Eastman Tritan TX1501HF Copolyester Eastman Tritan TX1501HF is a high flow grade of Eastman Tritan. Eastman Tritan TX1501HF has viscosity reductions of 40-50% relative to Eastman Tritan copolyester TX1001. Eastman Tritan copolyester.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Eastman Tritan WX500 Copolyester Eastman Tritan WX500 is a resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. This new-generati.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics GELOY CR7500 ASA (Asia Pacific) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Kleerdex Kydex® 101 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Thermoplastic sheet for signageApplications: Sign applications, radomes, other applications where a weatherable color over a white substrate is desirableFeatures: Kydex 101 is more rigid than most o.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Kleerdex Kydex® 120 Acrylic/PVC Thermoplastic Sheet
(discontinued **) USDA approved thermoplastic sheetApplications: High impact resistant wallcovering, push plates and kick plates, equipment housings, splash and safety guardsFeatures: Kydex 120 meets class I/A fire c.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Kleerdex Kydex® 150 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Class I/A rated thermoplastic sheetApplications: Interior ductwork and chutes, laboratory hoods, shower/tub shrouds, acoustical applications, decorative ceilings, abuse resistant surfacing for count.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | ASTM D790 |
Kleerdex Kydex® 550 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Weatherable monolithic sheetApplications: Housings for equipment, recreational vehicles and truck parts, safety equipment, building products, signageFeatures: Kydex 550 offers the properties of "Kyd.. |
|||
Flexural Yield Strength | 64.0 MPa | 9280 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp FF006 PE LNP Thermocomp FF-1006 is a glass filled Polyethylene.This data was supplied by SABIC-IP for the Americas region. |