| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
PolyOne Nymax™ 1010 A Black 13 Polyamide 6 (Nylon 6)
The Nymax® Series of nylon 6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of ..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN
SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Cycolac® INP572 ABS
High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
Network Polymers SAN 278 Medium Blue Tint
Description: SAN - Styrene Acrylonitrile Transparent Engineering ThermoplasticInformation provided by Network Polymers Inc.
|
|||
| Specific Gravity |
1.08
g/cc @Temperature 23.0 °C |
1.08
g/cc @Temperature 73.4 °F |
ASTM D792 |
|
Kingfa FRHIPS-1162 Flame Retardant Polystyrene
Features:UL 94 V-2 @ 1.6mm, V-2 @ 3.2mmExcellent balance properties, high strengthExcellent heat stabilityExcellent electrical propertiesApplications:Injection moldingGas moldingTV & Audio housingEl..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | |
|
Kuraray Genestarâ„¢ N1001D-U83/02 Nylon
Standard unreinforced extrusion grade. Main Features:Outstanding fuel barrierHeat resistanceExample of applications:Multi-layered fuel tube
|
|||
| Specific Gravity |
1.08
g/cc @Temperature 22.8 °C |
1.08
g/cc @Temperature 73.0 °F |
ASTM D792 |
|
Spartech PP5321 Mica Reinforced Homopolymer
Information provided by Spartech
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL GTX GTX902 PPE+PS+PA (Asia Pacific)
Unreinforced. Excellent chemical resistance and paintability. 312F (155C) HDT.
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL GTX GTX989 PPE+PA (Europe-Africa-Middle East)
NORYL GTX989 is a conductive and high heat material, especially designed for in- and on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D 792 |
|
SABIC Innovative Plastics Noryl N190A PPE+PS (Asia Pacific)
Low heat, flame retardant PPO/HIPS alloy. Internal flammability results only.Not a UL recognised material.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL NH5120C PPE+PS
Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The ..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Europe-Africa-Middle East)
Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The ..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled
Information from Shinkong Synthetic Fibers Corp.
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL EXNL0357 PPE+PS |
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL N1052P PPE+HIPS (Asia Pacific)
PPE+PS 105deg.C FR V-2
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer
DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
A. Schulman POLYFORT™ FPP 3391 Chemically Coupled, Modified Polypropylene
DescriptionPolyfort® FPP 3391 is a chemically coupled, mineral reinforced high impact resistant, modified polypropylene.Information provided by A. Schulman.
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
A. Schulman POLYBATCH™ Green 3012E Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 3012E is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3012E is he..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
Ensinger NORYL® Polyphenylene oxide (PPO)
NORYL®, due to its inherent chemical composition, exhibits unusually low moisture absorption. Therefore, good electrical insulating properties are realized over a wide range of humidity and temper..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
Ensinger TECANYL™ MT XRO Autoclavable Polymer
TECANYL™ MT is a new family of autoclavable materials developed for medical device applications. The material offers the desired performance properties of PPSU based resins with the machining ease..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
Diamond Polymers SAN 250 with Lube Styrene Acrylonitrile, Transparent Engineering Thermoplastic
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
Clariant Renol PA1SP0003 Nylon 66, PE Modified
Reduced Coefficient of FrictionData provided by Clariant Masterbatches
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
Bhansali Engineering Abstron TIM 300 MMA- ABS
High Impact(Transparent ABS)Information provided by Bhansali
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | 23°C; ASTM D792 |
|
Asahi Kasei Xyron® 340V Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | 23°C; ASTM D792 |
|
Asahi Kasei Xyron® 540Z Modified Polyphenylene Ether
Flame RetardantInformation provided by Asahi Kasei
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
BLUESTAR LXS 112 PPE-PS
Typical Applications: PV Industrial partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ISO 1183/1 |
|
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap..
|
|||
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
|
SABIC Innovative Plastics NORYL 115 PPE+HIPS (Asia Pacific)
PPE+PS, 115 oC HDT
|
|||