Polymer Property : Tensile Strength, Yield = 43.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 43.0 MPa
6240 psi
50 mm/min; ASTM D 638
Polimeri Europa Sinkral® C 442 ABS Resin
Sinkral C 442 is a heat resistant injection molding grade offering good flow and impact resistance together with excellent thermal stability during processing. Designation: Thermoplastic ISO 2580-AB..
Tensile Strength, Yield 43.0 MPa
6240 psi
50 mm/min; ISO 527
SABIC Innovative Plastics GELOY CR8510 ASA (Asia Pacific)
ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated.
Tensile Strength, Yield 43.0 MPa
6240 psi
50 mm/min
Polimeri Europa SINKRAL A22V ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-09-25 Very high flow grade for fast cycle injection moulding. Particularly recommended for the domestic ..
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527
GEHR Plastics POM-10PE Acetal Copolymer
Polyoxymethylene can be used in temperatures up to 100°C. The high surface strength is only surpassed by a few materials. POM shows good sliding properties and high resistance to wear and tear be..
Tensile Strength, Yield 43.0 MPa
6240 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC
LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated.
Tensile Strength, Yield 43.0 MPa
6240 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Asia Pacific)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Tensile Strength, Yield 43.0 MPa
6240 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East)
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Tensile Strength, Yield 43.0 MPa
6240 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT
LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.This data was suppl..
Tensile Strength, Yield 43.0 MPa
6240 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON DX93500 PC
LNP STAT-KON* DX93500 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Strength, Yield 43.0 MPa
6240 psi
ASTM D638
SABIC Innovative Plastics LNP STAT-KON SX90398 PA 12
LNP STAT-KON* SX90398 is a compound based on Nylon 12 resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS
LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant.
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527
Styrolution Novodur® 640 ABS
Novodur 640 is an injection molding grade of ABS with high impact strength and high gloss.Information provided by Styrolution
Tensile Strength, Yield 43.0 MPa
6240 psi
50mm/min; ISO 527
Styrolution Terblend® N NM-11 ABS/PA6 (Dry)
Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which..
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527-1/-2
Styrolution Terblend® N NM-19 XP Beige 38163 ABS+PA (Dry)
Description: Terblend® N NM-19 XP is an UV stabilized ABS/PA blend combining very high impact strength, even at low temperatures with an outstanding processability and excellent surface appearanc..
Tensile Strength, Yield 43.0 MPa
6240 psi
2 in/min; ASTM Test
Styrolution Terluran® HI-10 ABS
Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Tensile Strength, Yield 43.0 MPa
6240 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL WCV072 PPE+PP
Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De..
Tensile Strength, Yield 43.0 MPa
6240 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP STAT-LOY KX01002 Acetal Copolymer (Europe-Africa-Middle East)
LNP* Stat-Loy* KX01002 is a compound based on Acetal Copolymer resin containing Antistat. Added features include: Permanent Anti-Static.
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS
LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity.
Tensile Strength, Yield 43.0 MPa
6240 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP MF002AS PP
LNP THERMOCOMP* MF002AS is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized.
Tensile Strength, Yield 43.0 MPa
6240 psi
ASTM D638
Eastman Tritan MX711 Copolyester
Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co..
Tensile Strength, Yield 43.0 MPa
6240 psi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® RS LC1010 NC010 Nylon 1010  (Unverified Data**)
Unreinforced Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. ..
Tensile Strength, Yield 43.0 MPa
6240 psi
Fainplast Compounds R 220 Rigid PVC, Extrusion
Rolling shutters
Tensile Strength, Yield 43.0 MPa
6240 psi
Fainplast Compounds R 316/AS Rigid PVC, Extrusion
Antistatic profiles
Tensile Strength, Yield 43.0 MPa
6240 psi
50 mm/min
Arkema Group Rilsan® BMF Nylon 11 (Dry)
Designation ISO 1874-PA11,M,12-010Rigid grade for injection molding. Available color: natural. Additive free.Good melt viscosity. Outstanding ability to mold part with high length-thickness ratio an..
Tensile Strength, Yield 43.0 MPa
6240 psi
50mm/min; ISO 527
BASF Ultramid® 8202C PA6 (Conditioned)
Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique ..
Tensile Strength, Yield 43.0 MPa
6240 psi
2 in/min; ASTM Test
BASF Ultramid® 8202CQ PA6 (Conditioned)
Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme..
Tensile Strength, Yield 43.0 MPa
6240 psi
23°C, 50% RH; ASTM D638
Asahi Kasei Xyron® X0715 Modified Polyphenylene Ether
AutomotiveInformation provided by Asahi Kasei
Tensile Strength, Yield 43.0 MPa
6240 psi
ISO 527-2
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Tensile Strength, Yield 43.0 MPa
6240 psi
Type I, 50 mm/min; ASTM D638
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East)
Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen..
Tensile Strength, Yield 43.0 MPa
6240 psi
ASTM D638
BP Amoco Accpro® 9346 Enhanced Polypropylene  (discontinued **)
Suggested fabrication methods: Injection moldingFeatures: Long-term heat aging, High stiffness, Nucleated, UL RecognizedComplies with FDA specification, Title 21, CFR 177.1520.Typical applications: ..